Ing,
We only use a slow speed saw.
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
Sent: Wednesday, November 25, 2009 11:03 AM
To: [log in to unmask]
Subject: [TN] Preparing for microvia examination
Schrekxscht!
That was the way the aliens from planet Mars saluted us in the funny
film
that ended in their heads exploding when a guy played Elvis Presley on
his
car radio. What does that have to do with microvias? Anyone with
experience
from cutting a board into small pieces and mold them in epoxy for cross
section analysis? I use a thin blade, high rpm diamond blade for
cutting.
The board was equipped with SuperBGAs down to smallest QFNs. We
suspected
via problems and looked for such after polishing. In fact we found
extremly
good barrels and no sign of via issues. Instead we saw that some
cross-sectioned semi chips had fine microcracks. In some cases, the
microcrack ran all the way across the chip, i.e. the whole active area
was
more or less separated from the rest of the chip.My q is this: has
anyone
of you got microcracks in the semi chips caused during the cutting
operation? I,ve cross sectioned hundreds of boards during my time here,
but
never seen cracks like these be caused by the diamond cutting. Can there
be
a Schrekxscht when you use the diamond saw?
/Inge
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|