I think it will be machine specific and setup specific (diameter/type of
nozzle), the more free space the better. Depending on machine,
overtravel is sometimes used to prevent bridges when soldering rows of
pins. Another thing to look at is passive orientation w.r.t. the
selective solder nozzle. Parts running parallel with both terminations
potentially reflowing can be washed off whereas on perpendicular
oriented parts only one joint reflows and the part stays in place.
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson
Sent: Monday, November 16, 2009 11:01 AM
To: [log in to unmask]
Subject: [TN] Selective Soldering Nozzle Clearance
Greetings,
For anyone who does selective soldering:
I need to design a circuit board that has a few through-hole parts that
will
be soldered using a selective soldering machine, but I haven't found out
exactly which one it is yet (ELSA). Is there a DEFAULT clearance I
should
keep my SMT parts away from those Through-Hole pins, or do I really have
to customize it per machine?
thanks,
Jack (aka "the new guy")
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|