Like the gold if I can afford it. Super rich boss required. 4N the better. Ribbons are nicer.
--------------------------
Sent using BlackBerry
----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Fri Oct 30 09:39:47 2009
Subject: Re: [TN] Al wire bonding
Joyce,
Inge always comes up with the interesting comments, doesn't he!
He is such a gentlemen! I was thinking more of a foot being placed
somewhere else....
I shoot for medium Phos at ~5-8%. I believe that the medium Phos is most
typical anyway ....? [real plating guru's care to chime in on that
comment?].
My 'interest' with wedge bonding has always been focused around adequate
clamping of the part to prevent undue over/under bonding, or bond variation
and associated heel cracks, etc.
I understand what you said about matching hardness of the plating with the
wire, etc. The situations I have encountered with hybrids, however, is that
there are multiple different die metallization schemes with resulting
'hardness' characteristics that make matching die, wire, and PWB really hard
to do except for the simplest of configurations [ie - single chip modules].
Within reason I try to match to some extent, but I don't go over-board with
that concept [due to nature of parts primarily].
To some extent, gold ball bonding is a more forgiving process - don't you
agree!
Steve C
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
Sent: Friday, October 30, 2009 7:42 AM
To: [log in to unmask]
Subject: Re: [TN] Al wire bonding
IngeMar, what is the P content you target it too? 8%? Did you get any eye?
In the process to select a vendor? How many eyes?
--------------------------
Sent using BlackBerry
----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Fri Oct 30 02:42:05 2009
Subject: Re: [TN] Al wire bonding
I like the thumb in the supplier's eye bit. :-)
Anil
-----Original Message-----
From: Inge [mailto:[log in to unmask]]
Sent: Thursday, October 29, 2009 22:06
Subject: Re: Al wire bonding
Seconding what the best guru in America on bonding said. We have produced
millions of boards with Al wire on ENIG for years. Works just fine IF you
have the thumb in the board supplier's eye and do sample testing regularly
(coupon test).
/Inge
----- Original Message -----
From: "Jason Zhao" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, October 29, 2009 2:50 PM
Subject: Re: [TN] Al wire bonding
Interesting. I always think gold is the functional layer and the nickel is
there to prevent the copper migration to gold layers.
Regards,
Jason Zhao
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
Sent: Thursday, October 29, 2009 7:13 AM
To: [log in to unmask]
Subject: Re: [TN] Al wire bonding
Anat,
One can bond to the nickel [without the gold]!! This become especially easy
with heavier wire sizes [>2 mil].
Typically, one uses an ENIG plating. The immersion gold results in a gold
flash of ~2-5µinches
The gold is merely there to protect the nickel from oxidizing too much. One
actually bonds 'through' the gold layer to get to the underlying nickel.
If given a choice, I like pure soft gold instead of a hardened gold. If you
use ENIG, you may not get much choice in your gold.
It is my opinion that the thermal history & chronology of the board has more
of an inpact on wire bond reliability than simple plating. Eg - if one were
to reflow the board, [maybe] clean it, then let it set in que for multiple
weeks in a shop environment - I virtually guarantee you that you will note
differences in bonding characteristics as compared to a virgin board.
ENIG, or gold flash, is my answer. Keep them moving - don't let them set
around, is my recommendation.
Steve Creswick
On Thu, Oct 29, 2009 at 3:38 AM, Anat Douek <[log in to unmask]> wrote:
>
>
> Hi,
> What is the min gold thickness required for reliable aluminum wire bonding
> ?
> Which gold type is prefered for this process?
> It is needed for a military application.
>
> Regards,
> Anat Douek
> Process Engineer
> Herley General Microwave Israel
> tel. 972-25689455
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16for additional information,
or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|