Scott:
Attached files get dropped from TechNet. You will need to send it to Steve Gregory our picture/video librarian.
Gregg Owens
Technical Writer - Avionics
Space Exploration Technologies Corporation
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Post, Scott E
Sent: Wednesday, October 28, 2009 11:17 AM
To: [log in to unmask]
Subject: Re: [TN] Birth of a Solderball
We caught this on video a few years ago. It got rid of the notion we had
that placement pressure was squeezing paste out. The paste begins moving
under the part a few seconds before it's even molten.
Scott Post
P.O.U. 0000-001E-0CTC
2151 E. Lincoln Road
Kokomo, Indiana 46904-9005
765-451-2983 (Phone)
765-451-0287 (FAX)
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Wednesday, October 28, 2009 1:33 PM
To: [log in to unmask]
Subject: Re: [TN] Birth of a Solderball
If you have components with large flat terminations with respect to the
component height (even some 0805s can fall into this category) the
hydraulics required to overcome the resistance to wetting up the sides
of the terminations can cause a certain amount of backpressure, and thus
the solderballs. They squeeze out from under the chip caps, resistors,
and other components with much larger pad or land width with respect to
height. This is because these components are often printed using a 1:1
aperture/pad ratio. When solder paste melts, it needs some room to wet
out. This is why if you attempt to print paste on a "belly pad" QFN
without using at least a 50% aperture redux, the results can be
disastrous.
With the advent of Sn99 component finishes, I have noticed that the chip
cap/resistor's solderability shelf life is reduced due to a faster
oxidation rate. This exacerbates the issue somewhat.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gabriela
Sent: Wednesday, October 28, 2009 12:16 PM
To: [log in to unmask]
Subject: Re: [TN] Birth of a Solderball
Well, taking the subject of the letters 'mot a mot', I can give you an
example of "real" birth of solder balls.
HASL coated boards with defective tenting (due to artwork or
workmanship)
can contain excess of solder in the via holes- not blown out by the air
during HASL.
If you reflow the first side , the solder extrudes on the opposite side
through the small opening of the tenting and it really looks as if the
via gave birth to the small solder ball.
These small balls may stay in place or can be removed depending of the
surface they decided to stay.
Printing the second side with such babies causes shorts on fine pitch
components , not so much because of the balls, as because the paste
excess-
the stencil is not flat on the board.
Real Nightmare.
Want some pictures?
Gaby
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Wednesday, October 28, 2009 6:15 PM
To: [log in to unmask]
Subject: Re: [TN] Birth of a Solderball
Hi Leland - you would need to use analytical techniques for
micro-elemental analysis such as Scanning Transmission electron
microscopy or Atomic Force microscopy and there is no guarantee that the
resulting data would provide a source root cause (plus these techniques
are big bucks). Some of the other recommendations from the TechNet crew
are much
more practical.
Dave
"Leland Woodall" <[log in to unmask]>
10/28/2009 09:05 AM
To
"TechNet E-Mail Forum" <[log in to unmask]>, <[log in to unmask]>
cc
Subject
RE: [TN] Birth of a Solderball
Hi Dave,
Just how many thousands of dollars would that cost, and to what kind of
testing do you refer?
And I really didn't want to perform a cross section as well, so that was
good news!
Leland
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Wednesday, October 28, 2009 8:50 AM
To: [log in to unmask]
Subject: Re: [TN] Birth of a Solderball
Hi Leland - It may come as a surprise to many engineers but many metal
alloys actually have a "DNA" which can be traced back to original
processes and/or original sources. Unfortunately, unless you can find an
elemental signature difference in the solder alloy you use in your wave
solder process versus your reflow process (which you will need something
more sophisticated that standard SEM assessment) you will not be able to
determine which process may have produced the solder ball. I don't
believe that cross-sectional analysis will be beneficial unless you have
some baseline for comparison.
Dave Hillman
Rockwell Collins
[log in to unmask]
Leland Woodall <[log in to unmask]> Sent by: TechNet
<[log in to unmask]>
10/28/2009 06:54 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to Leland Woodall
<[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Birth of a Solderball
TechNetters,
Is there any possible way to determine the origin of a solder ball?
We've had a failure because of one, and we're trying to determine
whether it came from our SMT or wave soldering process.
We use SAC305 at both, so using the SEM to determine alloy composition
is not really helping.
The ball itself is spherical with no "tails" and quite shiny in
appearance.
If we cross section the ball, will we see a difference in grain
structure due to the differences in cool down rates? Is there anything
else we can use or do?
Thanks in advance for your help!
Leland
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
************************************************************************
****************
Note: If the reader of this message is not the intended recipient, or
an employee or agent responsible for delivering this message to the
intended recipient, you are hereby notified that any dissemination,
distribution or copying of this communication is strictly prohibited. If
you have received this communication in error, please notify us
immediately by replying to the message and deleting it from your
computer. Thank you.
************************************************************************
****************
****************************************************************************************
Note: If the reader of this message is not the intended recipient, or an employee or agent responsible for delivering this message to the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify us immediately by replying to the message and deleting it from your computer. Thank you.
****************************************************************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|