Richard,
We cover all of assemblies before sending them through the wave. We did
this in order to eliminate the spatters.
We were also able to re-create the handling transfer yesterday. Given
the correct combination of ball size and component spacing, surprisingly
little force is required to wedge the ball and slightly flatten the
sides.
Leland
-----Original Message-----
From: Stadem, Richard D. [mailto:[log in to unmask]]
Sent: Wednesday, October 28, 2009 10:07 AM
To: TechNet E-Mail Forum; Leland Woodall
Subject: RE: [TN] Birth of a Solderball
Probably a spattered sphere. It would take a lot of force to flatten the
sides of a SAC305 or similar solderball.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
Sent: Wednesday, October 28, 2009 8:58 AM
To: [log in to unmask]
Subject: Re: [TN] Birth of a Solderball
Jowan,
The solderball that caused the failure was wedged on top of and between
two adjacent chip capacitor terminations. The solderball looked as if
it had been pressed downward, as there were two slightly flat surfaces
that were evident upon removal.
So, really, the location of the failure didn't give us much of a clue
toward its origin.
At this point, we can venture that the ball migrated there from
associate handling. We're just trying to understand which process
generated the actual formation...
Leland
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Iven, Jowan
Sent: Wednesday, October 28, 2009 9:06 AM
To: [log in to unmask]
Subject: Re: [TN] Birth of a Solderball
Hi Leland,
What about the location of the solderball?
Doesn't that give you enough information?
Where on the board was the solderball located?
Or did the problem occur somewere else but the board?
Jowan
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
Sent: Wednesday, October 28, 2009 12:54 PM
To: [log in to unmask]
Subject: Birth of a Solderball
TechNetters,
Is there any possible way to determine the origin of a solder ball?
We've had a failure because of one, and we're trying to determine
whether it came from our SMT or wave soldering process.
We use SAC305 at both, so using the SEM to determine alloy composition
is not really helping.
The ball itself is spherical with no "tails" and quite shiny in
appearance.
If we cross section the ball, will we see a difference in grain
structure due to the differences in cool down rates? Is there anything
else we can use or do?
Thanks in advance for your help!
Leland
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
This e-mail and any attachment is confidential and may be legally
privileged or otherwise protected from disclosure. If you are not the
intended recipient, please notify the sender immediately by returning
this e-mail. Neways Electronics NV is not responsible for the improper
or incomplete transmission of any e-mail, or for any delay in its
receipt.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|