Anat,
One can bond to the nickel [without the gold]!! This become especially easy
with heavier wire sizes [>2 mil].
Typically, one uses an ENIG plating. The immersion gold results in a gold
flash of ~2-5µinches
The gold is merely there to protect the nickel from oxidizing too much. One
actually bonds 'through' the gold layer to get to the underlying nickel.
If given a choice, I like pure soft gold instead of a hardened gold. If you
use ENIG, you may not get much choice in your gold.
It is my opinion that the thermal history & chronology of the board has more
of an inpact on wire bond reliability than simple plating. Eg - if one were
to reflow the board, [maybe] clean it, then let it set in que for multiple
weeks in a shop environment - I virtually guarantee you that you will note
differences in bonding characteristics as compared to a virgin board.
ENIG, or gold flash, is my answer. Keep them moving - don't let them set
around, is my recommendation.
Steve Creswick
On Thu, Oct 29, 2009 at 3:38 AM, Anat Douek <[log in to unmask]> wrote:
>
>
> Hi,
> What is the min gold thickness required for reliable aluminum wire bonding
> ?
> Which gold type is prefered for this process?
> It is needed for a military application.
>
> Regards,
> Anat Douek
> Process Engineer
> Herley General Microwave Israel
> tel. 972-25689455
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|