TECHNET Archives

October 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 26 Oct 2009 09:53:20 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Hernefjord Ingemar <[log in to unmask]>
Subject:
From:
Hernefjord Ingemar <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
<51733F7A39D14A58854571F17A3F97F5@StephenPC>
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (133 lines)
 Manuel,

there are several things that seem anomalous:
1. Looks like Copper is exposed at the end of some leads. Gives the impression of poor lead finish.
2. The solder spheres are not fully melted at the outermost part of the solder pad. Due to short top temp zone exposure?
3. Some solder pads are not wetted 100% or have dewetted. Looks like bad finish.
4. The solder mask is very close to the solder pads. Maybe you get solder mask contaminations on the solder pads.
5. The leads seem to be lifted during the soldering process.
6. Youd can't see the whole solder joint. Is the innermost part of the solder joints as bad as the outermost ones?
7. The colour of the non-wetted ( or de-wetted )part of the solder pads tells me that the solder pad finish is bad.

I've never seen so many divergences at one and the same positions. A first look gives the impression that the solder paste was bad, that the lead finish was bad, that the solder pad finish was bad and that the soldering process was incorrect. Of course that's not a correct analysis. Question is which one is the bad guy. I suspect that not even the TN gurus can decide without knowing a little more. E.g. what soldering process was used? What solder paste? How do the other component's SJs look like? What's the size of the board? What mass? What pre-clean process? What stencil thickness? Etc. 

If I do my best guessing, I vote for local poor solder pad finish. I will enjoy reading the correct analysis later from someone of the heavyweighters in the game...

/Inge


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of stephengregory5849
Sent: måndag 26 oktober 2009 02:41
To: [log in to unmask]
Subject: Re: [TN] Questions

Hi Manuel,

I'm sorry I didn't get your pictures posted sooner, but I have them up now, and I'm posting everything to the TechNet for you. Your pictures are here:

http://stevezeva.homestead.com/1a.JPG

http://stevezeva.homestead.com/2a.JPG

http://stevezeva.homestead.com/3a.JPG

http://stevezeva.homestead.com/5a.JPG

I posted the pictures that looked the best to illustrate your problem, a couple of pictures were out of focus and it was hard to see the problem.

Were the IC's the only component that had this problem? That pretty much eliminates the solderpaste if it was. It makes it harder to figure out when you say that it was random and only on three boards. What was the lead finsh on the IC's? I've had a few problems with lead-free (tin) plating, but it's been with connectors.

Steve
  ----- Original Message -----
  From: Manuel Castro
  To: [log in to unmask] ; Werner Engelmaier
  Sent: Friday, October 23, 2009 7:00 PM
  Subject: Re: Questions


  Steven,

  Attached are the photos of the issues. We run this assembly through our SMT oven and got a few boards (3) with this phenomenon at some of the leads on this FPIC. The IC was the same part number but the location was random on all 3 boards. The chemistry utilize during this build was Lead Free NC. 

  How do I send the email to everyone at the TechNet forum?...


  Thank you All...


  Best regards,

  Manuel Castro Jr.
  Senior Process Engineering Manager
  [log in to unmask]
  Office: (408) 964-3044
  Fax: (408) 964-3001





  On Fri, Oct 23, 2009 at 1:14 PM, Werner Engelmaier <[log in to unmask]> wrote:



    Hi Manuel,
    Steven is the GOOD guy doing the posting on his website-he recently changed jobs, e-mails, etc.; so it might be best to ask him directly.
    Werner



    -----Original Message-----
    From: Manuel Castro <[log in to unmask]>
    To: [log in to unmask]
    Sent: Fri, Oct 23, 2009 1:11 pm
    Subject: Questions


    Hi Werner,

    I love to follow all TechNet forum but I still don't know where the picture get posted from everyone that has an issue. Can you kindly tell me what the link is. Do we need a password to access the pictures. Lastly, if I have an issue where do I post the picture to share with the team or whom do I sent it to?



    Best regards,

    Manuel Castro Jr.
    Senior Process Engineering Manager
    [log in to unmask]
    Office: (408) 964-3044
    Fax: (408) 964-3001



CONFIDENTIALITY
This e-mail message and any attachments thereto, is intended only for use by the addressee(s) named herein and may contain legally privileged and/or confidential information. If you are not the intended recipient of this e-mail message, you are hereby notified that any dissemination, distribution or copying of this e-mail message, and any attachments thereto, is strictly prohibited.  If you have received this e-mail message in error, please immediately notify the sender and permanently delete the original and any copies of this email and any prints thereof.


ABSENT AN EXPRESS STATEMENT TO THE CONTRARY HEREINABOVE, THIS E-MAIL IS NOT INTENDED AS A SUBSTITUTE FOR A WRITING.  Notwithstanding the Uniform Electronic Transactions Act or the applicability of any other law of similar substance and effect, absent an express statement to the contrary hereinabove, this e-mail message its contents, and any attachments hereto are not intended to represent an offer or acceptance to enter into a contract and are not otherwise intended to bind the sender, Sanmina-SCI Corporation (or any of its subsidiaries), or any other person or entity.






CONFIDENTIALITY
This e-mail message and any attachments thereto, is intended only for use by the addressee(s) named herein and may contain legally privileged and/or confidential information. If you are not the intended recipient of this e-mail message, you are hereby notified that any dissemination, distribution or copying of this e-mail message, and any attachments thereto, is strictly prohibited.  If you have received this e-mail message in error, please immediately notify the sender and permanently delete the original and any copies of this email and any prints thereof.
ABSENT AN EXPRESS STATEMENT TO THE CONTRARY HEREINABOVE, THIS E-MAIL IS NOT INTENDED AS A SUBSTITUTE FOR A WRITING.  Notwithstanding the Uniform Electronic Transactions Act or the applicability of any other law of similar substance and effect, absent an express statement to the contrary hereinabove, this e-mail message its contents, and any attachments hereto are not intended to represent an offer or acceptance to enter into a contract and are not otherwise intended to bind the sender, Sanmina-SCI Corporation (or any of its subsidiaries), or any other person or entity.


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2