Should inspect on the solder joints of these rejects, you will able to
know that touch/rework had been done on these pins.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Edwards
Sent: Thursday, 8 October 2009 1:14 AM
To: [log in to unmask]
Subject: Re: [TN] gold connector discoloration
I agree with Victor on the solder-on-Au-connector issue...
Looks to me that someone either reworked or touched-up the connectors
after SMT or they hand soldered the connectors in...
Adding flux to the connector and touching the SJs to clear a solder
short or (most likely) to add solder to the joint will cause solder to
wet up into the contact area on low profile connectors...Extra heat
starts it but too much solder and flux does it every time...
You'll have to ask the CM to remove and replace the connectors...
Paul
Paul Edwards
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Wednesday, October 07, 2009 10:06 AM
To: [log in to unmask]
Subject: Re: [TN] gold connector discoloration
Beware of fretting with the solder on the gold plated contacts.
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gumpert, Ben
Sent: Wednesday, October 07, 2009 9:34 AM
To: [log in to unmask]
Subject: Re: [TN] gold connector discoloration
Justin,
It looks like you have some solder that has made its way up the gold.
The picture of the prior board looked as if there was less solder used
to attach the connector, as there is still evidence of gold on the leads
(where solder has not covered the leads as it has done in the 'new
batch' image).
Maybe they installed connectors that had been tinned, so there was
additional solder in the process.
Ben
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Justin Braime
Sent: Wednesday, October 07, 2009 10:12 AM
To: [log in to unmask]
Subject: [TN] gold connector discoloration
Hi Technetters,
We've just received a new batch of boards from one of our
subcontractors,
and the Hirose DF12 header sockets have discoloration on the mating
terminals.
On previous batches, we have seen a little discoloration adjacent to the
solder joints, but never up in the connector mating area itself. The
process
hasn't (allegedly) changed.
I've posted some pics at:
http://gallery.me.com/jbraime/100005
Any ideas as to the cause? Any detriment to functionality?
Thanks in advance,
Justin
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please visit http://www.messagelabs.com/email
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
========================================================================
======
This email and any attachments thereto may contain private,
confidential, and
privileged material for the sole use of the intended recipient. Any
review, copying,
or distribution of this email (or any attachments thereto) by others is
strictly prohibited.
If you are not the intended recipient, please contact
[log in to unmask]
immediately and permanently delete the original and any copies of this
email and
any attachments thereto.
========================================================================
======
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|