Request the biggest aperture opening of your stencil from you supplier. Measure it thickness, this is the way we inspect for the thickness of the stencil foil. Or you can ask/design to cut out more opening at different locations of your stencil to ensure/study the evenness of the thickness.
________________________________
From: TechNet on behalf of Glidden, Kevin
Sent: Thu 10/15/2009 3:32 AM
To: [log in to unmask]
Subject: Re: [TN] Stencil Thickness Verification
The stands usually have a mount that allows you to bolt through to the indicator.
-----Original Message-----
From: Leland Woodall [mailto:[log in to unmask]]
Sent: Wednesday, October 14, 2009 2:22 PM
To: TechNet E-Mail Forum; Glidden, Kevin
Subject: RE: [TN] Stencil Thickness Verification
Now I'm getting the picture. We're after the foil thickness, and the
way you suggest below I believe would work. I just have to figure out
how to rig up the device.
As for the first part of my question, I guess no one actually performs a
thickness verification of their incoming framed stencils (or if they do,
they don't subscribe to this forum).
Thanks, everyone, for your input!
Leland
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glidden, Kevin
Sent: Wednesday, October 14, 2009 1:54 PM
To: [log in to unmask]
Subject: Re: [TN] Stencil Thickness Verification
Are you looking to measure foil thickess or etched aperture depth?
Using an indicator, you would mount it to a stand / surface plate, then
you zero the indicator on the plate surface, then place the foil on the
surface and indicate to the top surface of the foil. This will give you
the foil thickness.
-----Original Message-----
From: Leland Woodall [mailto:[log in to unmask]]
Sent: Wednesday, October 14, 2009 1:42 PM
To: Glidden, Kevin; TechNet E-Mail Forum
Subject: RE: [TN] Stencil Thickness Verification
Kevin,
I looked at that device online, and can't understand how I could use it
to check the depth of an aperture. What am I missing?
Leland
-----Original Message-----
From: Glidden, Kevin [mailto:[log in to unmask]]
Sent: Wednesday, October 14, 2009 1:35 PM
To: TechNet E-Mail Forum; Leland Woodall
Subject: RE: [TN] Stencil Thickness Verification
Wouldn't a standard drop gage suffice?
For example, mitutoyo p/n 1923 in a range of 0 - .05 in, .0005
graduations.
-----Original Message-----
From: Leland Woodall [mailto:[log in to unmask]]
Sent: Wednesday, October 14, 2009 1:22 PM
To: [log in to unmask]
Subject: [TN] Stencil Thickness Verification
TechNetters,
Does anyone in the industry verify their framed stencils for thickness
upon receipt at their facility? If so, could someone please share what
kind of tool they use?
I'm having difficulty finding such an animal that will accurately
distinguish between 5 and 6 mils.
Thanks for your help,
Leland
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|