Sender: |
|
X-To: |
|
Date: |
Fri, 9 Oct 2009 09:54:05 -0500 |
Reply-To: |
|
Subject: |
|
From: |
|
Content-Transfer-Encoding: |
quoted-printable |
In-Reply-To: |
|
Content-Type: |
text/plain; charset="us-ascii" |
MIME-Version: |
1.0 |
Parts/Attachments: |
|
|
Lee,
I would not have quit so easily. It is apparent that the Xzerbian aliens
did not want you to discover their secret for variable spectrum
propulsion. Thank God it's Friday!
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee parker
Sent: Friday, October 09, 2009 9:28 AM
To: [log in to unmask]
Subject: Re: [TN] Criteria for brightness of Hard Gold plating
Rudy
You may be correct. I had a boss once who purchased a very expensive
machine that collect the reflective light from a surface and the
decomposed the radiation into the primary colors. We spent a year trying
to find and application. Fortunately and curiously the machine broke
down and we were able to scrap it.
Best regards
Lee
J. L. Parker Ph. D.
JLP Consultants LLC
804 779 3389
----- Original Message -----
From: R Sedlak<mailto:[log in to unmask]>
To: TechNet E-Mail Forum<mailto:[log in to unmask]> ; Lee
parker<mailto:[log in to unmask]>
Sent: Friday, October 09, 2009 10:11 AM
Subject: Re: [TN] Criteria for brightness of Hard Gold plating
Sadly, the importance of this may well be determined merely by
the fact that the customer has an instrument which they feel they need
to justify the purchase of.
Rudy Sedlak
RD Chemical Company
--- On Fri, 10/9/09, Lee parker
<[log in to unmask]<mailto:[log in to unmask]>> wrote:
From: Lee parker <[log in to unmask]<mailto:[log in to unmask]>>
Subject: Re: [TN] Criteria for brightness of Hard Gold plating
To: [log in to unmask]
Date: Friday, October 9, 2009, 6:44 AM
I am curious, why is brightness important? The most
significant index is hardness and there are testing techniques that have
been accepted by the industry for many years.
Best regards
Lee
J. L. Parker Ph. D.
JLP Consultants LLC
804 779 3389
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|