Just out of curiosity, when you detect an open on a BGA, what do you do? I'm
suspecting it is not practical to rework just the open sj, can you reflow the
entire BGA to get the open sj to form a connection, or remove and reattach?
Do you re-use the removed device or replace with a new one?
Is the x-ray inspection really useful, or is it just to confirm a defect found in
test? Or does it detect defects before test so that they can be reworked prior
to testing?
Is the x-ray inspection useful for getting the profile parameters correct, and
then once the process is in control the inspection no longer adds value?
Thanks,
Blair
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|