Blair,
I have run hundreds of assemblies through Ionic testing.
1. I have discovered failures for no apparent reason and it turned out
to be the PCB's themselves. Now I have the PCB's tested when they are
fabricated (at the board shop) and have no more IONIC contamination
failures do to contamination at all.
2. Even though 100% of our boards are being tested for IONIC
contamination we have had a few boards hear and there that have failed
electrical testing because of flux entrapment under BGA's that are
around 1MM pitch. After removing the BGA it looks like a dark
gray\black blob of corrosion probably do to the power going through the
resistance of the flux and solder.
My suspicion is that the water molecules don't always make it under
BGA's to remove all of the flux from processing. Interesting though I
don't seem to have had problems with micro-BGA's.
One other point is that we use water soluble flux as a process and not
no-clean fluxes because of the appearance of our products.
Hope this helps,
Pete Siperek, IPC(CID+)
Sr. Staff Engineer
Delphi Engineering Group, Inc
phn 949-515-1490 ext. 478
fax 949-515-1491
[log in to unmask]
Your Partner in Product Development
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Blair Hogg
Sent: Friday, October 30, 2009 6:40 AM
To: [log in to unmask]
Subject: [TN] Cleanliness
A ROSE by any other name would smell as sweet, right SIR?
Happy Friday, Technetters! As you may have guessed, I've spent a bit of
time over the last few days looking over cleanliness testing specs,
searching through the archives and what not to get more information on
the different types of testing. Now it is time to visit the well of
knowledge and see if the Technet gurus can help me along the road to
cleanliness enlightenment.
From what I understand, the ROSE test measure the change in resisitivity
/ conductivity of a test solvent solution (75% IPA / 25% DI Water) that
is rinsed over a board / assembly. This will detect contaminants and
provide a relative level of the contamination. However, it will only
detect those contaminants that are ionic in nature or will affect the
resistivity (is that redundant?). The results are near immediate.
The SIR test measures the insulation resisitance change that occurs when
an assembly is exposed to humidity and voltage, and thus has the
capability of detcting the presence of contaminants that may not be
ionic, but can cause corrision and / or dendrites to grow. The drawback
is that the samples must be exposed to controlled humidity / temperature
for a priod of time.
Does that sound right? Am I missing anything?
Are there any other options?
Thanks,
Blair
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|