TECHNET Archives

October 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 26 Oct 2009 17:19:14 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Werner Engelmaier <[log in to unmask]>
Subject:
From:
Werner Engelmaier <[log in to unmask]>
Content-Type:
text/plain; charset="utf-8"
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
MIME-Version:
1.0
Parts/Attachments:
text/plain (174 lines)
 Anybody know what the material of these lead is? It may not be very solderable.
Werner

 

 

-----Original Message-----
From: Ioan Tempea <[log in to unmask]>
To: [log in to unmask]
Sent: Mon, Oct 26, 2009 3:39 pm
Subject: [TN] Stella's connector










Linda,

I've been through this ordeal with a different shape connector, but same pin 
layout. I couldn't fix it, but our production people tried some more and seen 
that if the connector is glued down at the corners with mold seal, just like the 
TH parts that must be prevented from lifting in wave, the problem goes away. I 
have no explanation for this, but it should be tried.

Good luck,

Ioan Tempea, ing.
t : 450-967-7100 ext : 244
[log in to unmask]
www.digico.cc
P N'imprimer que si nécessaire - Print only if you must
-----Message d'origine-----
De : Steve Gregory [mailto:[log in to unmask]] 
Envoyé : Monday, October 26, 2009 3:11 PM
À : [log in to unmask]
Objet : Re: [TN] Steve Gregory

Hi Linda,

I have the pictures posted. Here are the links:

http://stevezeva.homestead.com/crx_pre-sample_2.JPG


http://stevezeva.homestead.com/val10crx_overview.JPG


http://stevezeva.homestead.com/crz_pre-sample_2.JPG


http://stevezeva.homestead.com/val10crz_overview.JPG


http://stevezeva.homestead.com/crx_sample_2-x150.JPG


http://stevezeva.homestead.com/Stella_pic1.JPG


http://stevezeva.homestead.com/Stella_pic2.JPG

As far as measuring warpage during reflow, I found this:

http://www.malcomtech.com/Electronics/products_srs2.html



Never used one, never seen one used, so I can't vouch for it. But it does
look like a fun toy!

Steve

-----Original Message-----
From: Linda Langley [mailto:[log in to unmask]] 
Sent: Monday, October 26, 2009 7:23 AM
To: Steve Gregory
Subject: RE: [TN] Steve Gregory

Steve,
We hope to get some information for Stella.



Linda,

I know that you are signed on TechNet
Could you please post question to all experts for me:

We are reflowing 50pins CF card SMT connector and having high rate of the
lifted leads (they are gull wings leads). We measured leads coplanarity
using CMM before reflow and it seems that all leads are meeting the spec. 
My guess is that the component body is bowing during reflow process (we are
dong Pb free reflow with the peak of 234°C) causing lifted leads.
Somebody told me that there is a lab who can measure leads coplanarity
during reflow cycle. Is anybody aware of such as test?
Thank you

Stella Neyman

-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]] 
Sent: Monday, October 26, 2009 6:52 AM
To: Linda Langley
Subject: RE: [TN] Steve Gregory

Hi Linda,

Sure, send them my way...

Steve

-----Original Message-----
From: Linda Langley [mailto:[log in to unmask]] 
Sent: Monday, October 26, 2009 6:05 AM
To: [log in to unmask]
Subject: RE: [TN] Steve Gregory

Steve,
Will you be able to post my pictures?

Linda Langley CIT
Training Specialist
Jabil Circuit
248-292-6176

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------



 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2