TECHNET Archives

October 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 16 Oct 2009 11:10:02 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Linda Langley <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Linda Langley <[log in to unmask]>
Parts/Attachments:
text/plain (53 lines)
Steve,

I have a couple of pictures I would like for you to post, Stella would like to know if anyone has information about how to correct this problem.

 

 

 

Linda

I know that you are signed on Technet

Could you please post question to all experts for me:

We are reflowing 50pins CF card SMT connector and having high rate of the lifted leads (they are gull wings leads). We measured leads co planarity using CMM before reflow and it seems that all leads are meeting the spec. 

My guess is that the component body is bowing during reflow process (we are dong Pb free reflow with the peak of 234°C) causing lifted leads.

Somebody told me that there is a lab who can measure leads coplanarity during reflow cycle. Is anybody aware of such as test?

Thank you

 

 

Stella Neyman

 

 

Linda Langley CIT

Training Specialist

Jabil Circuit

248-292-6176


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2