HASL LF or SnPb 12 months
Imm. Ag, Imm Sn, OSP 6 months
ENIG 6 - 12 months
Best Regards
Reuven ROKAH
Think green before printing this mail... Thanks
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of ?efika ?zkal
Sent: Tuesday, September 08, 2009 8:24 AM
To: [log in to unmask]
Subject: [TN] shelf life of pcbs
Dear Technetters,
I would like to get information about shelf life of pcbs. I know they change
with the finish type of the pcbs but is there an IPC Standard which defines
the shelf life of pcbs for different finishes?
Thanks
Sefika Ozkal
ASELSAN INC.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of stephengregory5849
Sent: Sunday, September 06, 2009 3:31 AM
To: [log in to unmask]
Subject: Re: [TN] [LF] electronics recycling in China
Robin,
Thank you for sharing the "rest of the story". I watched the 60-minutes
story last Sunday, and was thinking that there wasn't any e-waste recycler
in the US that you could trust. You have totally changed what I now think.
Thank you, and kudos to you and Retroworks for what you do. I wish there
were more like you.
Steve Gregory
----- Original Message -----
From: "Robin Ingenthron" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Saturday, September 05, 2009 7:12 PM
Subject: Re: [LF] electronics recycling in China
> Bolb,
>
> Actually, I was interviewed for 3 hours but wasn't ultimately used as a
> source because a) it didn't fit in their 8 minutes, and b) Scott Pelley
> was
> really thrilled to have someone try to take his camera away.
>
> While the story is true, it omits a key step in the chain. * Here is the
> rest of the
>
story<http://retroworks.blogspot.com/2009/08/cbs-60-minutes-wasteland-unseen
-footage.html>.
> *
>
> On Sat, Sep 5, 2009 at 5:57 PM, Bob Landman
> <[log in to unmask]>wrote:
>
>> This piece on electronics recycling ran on 60 Minutes Sunday August 30,
>> 2009.
>> It's a repeat program that originally aired in November 2008.
>>
>> The Electronic Wasteland
>> http://www.cbsnews.com/video/watch/?id=4586903n
>>
>> This is the reason lead in solder is being banned.
>>
>> Instead of fixing the problem, a new one (lead free manufacturing) has
>> been
>> created.
>> The result (reduced reliability of electronics) will be far worse on
>> human
>> life (in toto)
>> than the pollution seen in this video, IMHO.
>>
>> Bob Landman, President
>> Life Senior Member, IEEE
>> IEEE Power & Energy/Reliability Societies
>> IEEE Standards Association
>> H&L Instruments, LLC
>> www.hlinstruments.com
>>
>>
----------------------------------------------------------------------------
---Leadfee
>> Mail List provided as a service by IPC using LISTSERV 1.8d
>> To unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Leadfree
>> To temporarily stop/(start) delivery of Leadree for vacation breaks send:
>> SET Leadfree NOMAIL/(MAIL)
>> Search previous postings at: http://listserv.ipc.org/archives
>> Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16for additional
>> information, or contact Keach Sasamori at
>> [log in to unmask] or 847-615-7100 ext.2815
>>
>>
----------------------------------------------------------------------------
---
>>
>
>
>
> --
> Robin Ingenthron
>
>
----------------------------------------------------------------------------
---Leadfee
> Mail List provided as a service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Leadfree
> To temporarily stop/(start) delivery of Leadree for vacation breaks send:
> SET Leadfree NOMAIL/(MAIL)
> Search previous postings at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
>
----------------------------------------------------------------------------
---
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
######################################################################
Dikkat:
Bu elektronik posta mesaji kisisel ve ozeldir. Eger size
gonderilmediyse lutfen gondericiyi bilgilendirip mesaji siliniz.
Firmamiza gelen ve giden mesajlar virus taramasindan gecirilmekte,
guvenlik nedeni ile kontrol edilerek saklanmaktadir. Mesajdaki
gorusler ve bakis acisi gondericiye ait olup Aselsan A.S. resmi
gorusu olmak zorunda degildir.
######################################################################
Attention:
This e-mail message is privileged and confidential. If you are
not the intended recipient please delete the message and notify
the sender. E-mails to and from the company are monitored for
operational reasons and in accordance with lawful business practices.
Any views or opinions presented are solely those of the author and
do not necessarily represent the views of the company.
######################################################################
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|