Paul,
I agree.
A week ago I asked what is it about HASL that causes problems, other than
less than perfectly flat pads. I don't recall seeing any answers.
With paste and machine placement the surface finish of the PCB does not
seem important, except for reflow quality. From what I read and my
experience with other finishes, HASL is about as good as you get for ease of
reflow.
Bob Kondner
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Edwards
Sent: Wednesday, September 30, 2009 1:28 PM
To: [log in to unmask]
Subject: Re: [TN] ENIG / HASL CO-PLANARITY
Why does this always come up?
With everything that is said about the real and potential metallurgical
problems with ENIG, how can ENIG be considered a good replacement for a
HASLed PCB, unless you are considering only the PCB fabrication of RoHS
boards or the bulk buying PCB materials ?
Look at the flatness numbers for HASLed PCBs...Unless you have huge pads and
a very bad PCB fabricator the HASL thickness variation is typically no more
than 0.0007" on standard part pads... That is better than the planarity on
everything but LCCs and QFN type structures and well within the solder paste
print height tolerances of most systems...
Besides the last time I checked we all put solder paste on pads before we
stuck parts to the PCB so there is at least 0.004" of solder compliance to
compensate for any bumping of the HASL...
Have built a lot of high-density high-rel PCAs and over a lot of years and I
will take a HASLed PCA over any other kind of surface finish...
Paul
Paul Edwards
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Wednesday, September 30, 2009 7:54 AM
To: [log in to unmask]
Subject: Re: [TN] ENIG / HASL CO-PLANARITY
Hi Lee - You might try another approach with the customer. Image that you
have a very large, nonflexible beach ball and you are trying to balance it
on your local parking lot speed bump - if you are using a HASL finish and
processing BGAs or CSPs you are doing the same procedure. Sometimes having
a visual reference is worth a pound of tolerance measurements. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Lee Whiteman <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
09/25/2009 09:09 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]
To
[log in to unmask]
cc
Subject
[TN] ENIG / HASL CO-PLANARITY
Happy Friday.
Does anyone have a reference on comparing the co-planarity between ENIG
and HASL (SnPb)? I know that ENIG is more planar than HASL, but by how
much (quantifying the argument). I'm anticipating a question from my
customer on why I want to use ENIG instead of HASL for fine pitch
applications.
Thanks.
Lee Whiteman, PMP
Senior Member Engineering Staff
L-3 Communications East
Telephone: (856) 338-3508
FAX: (856) 338-2906
E-Mail: [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
===========================================================================
==
This email and any attachments thereto may contain private, confidential,
and
privileged material for the sole use of the intended recipient. Any review,
copying,
or distribution of this email (or any attachments thereto) by others is
strictly prohibited.
If you are not the intended recipient, please contact
[log in to unmask]
immediately and permanently delete the original and any copies of this email
and
any attachments thereto.
===========================================================================
==
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|