Mike,
It is the standard 3M #250 tape and I agree any residue could be cleaned after testing.
Thanks,
Tom Carroll, CQA, CIT
Supplier Quality Engineer
Boeing Integrated Defense Systems - East Region Supplier Quality
Home Office Phone/FAX: 845-753-5932
Temp Office Phone at Alabama Aircraft Indus Inc (205) 510-4783
Temp Office FAX at AAII (205) 592-0295
Boeing Cell: 215-692-2463
email: [log in to unmask]
> NOTE: This communication may contain privileged or other confidential information. If you are not the intended recipient, or believe you have received this communication in error, please do not print, copy, retransmit, disseminate, or otherwise use the information. Also, please indicate to the sender that you have received this e-mail in error, and delete the copy you received. Thank you.
> EXPORT COMPLIANCE STATEMENT:
> "The information contained herein is or may be controlled by the International Traffic in Arms Regulations (ITAR), 22 CFR 120-130, and may not be exported, or disclosed to a foreign person, whether in the United States or abroad, without prior U.S. Government written approval"
-----Original Message-----
From: Mike Sewell [mailto:[log in to unmask]]
Sent: Thursday, September 24, 2009 8:04 AM
To: TechNet E-Mail Forum; Carroll, Thomas A
Subject: RE: [TN] Adhesion Testing of Brush Plating
If there is a residue left, can't they clean it? Sounds like they are trying to avoid an extra step (or two). What adhesive is on the tape they would use?
FWIW - The intended use of MIL-STD-865D is "...used during repair process and acquisition of spares for the landing gear of all military aircraft. It is a process and procedure unique to the Air Force and is used primarily by the Air Force at Hill Air Force Base."
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Carroll, Thomas A
Sent: Thursday, September 24, 2009 6:56 AM
To: [log in to unmask]
Subject: Re: [TN] Adhesion Testing of Brush Plating
Joyce,
The adhesion test should confirm that the brush plate process was performed correctly.
Regards,
Tom Carroll, CQA, CIT
Supplier Quality Engineer
Boeing Integrated Defense Systems - East Region Supplier Quality Home Office Phone/FAX: 845-753-5932 Temp Office Phone at Alabama Aircraft Indus Inc (205) 510-4783 Temp Office FAX at AAII (205) 592-0295 Boeing Cell: 215-692-2463
email: [log in to unmask]
> NOTE: This communication may contain privileged or other
confidential information. If you are not the intended recipient, or believe you have received this communication in error, please do not print, copy, retransmit, disseminate, or otherwise use the information.
Also, please indicate to the sender that you have received this e-mail in error, and delete the copy you received. Thank you.
> EXPORT COMPLIANCE STATEMENT:
> "The information contained herein is or may be controlled by the
International Traffic in Arms Regulations (ITAR), 22 CFR 120-130, and may not be exported, or disclosed to a foreign person, whether in the United States or abroad, without prior U.S. Government written approval"
-----Original Message-----
From: Joyce Koo [mailto:[log in to unmask]]
Sent: Wednesday, September 23, 2009 5:11 PM
To: TechNet E-Mail Forum; Carroll, Thomas A
Subject: RE: [TN] Adhesion Testing of Brush Plating
You mean no qual can be done? If it is the case, what is good for adhesion test if each of them are unique.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Carroll, Thomas A
Sent: Wednesday, September 23, 2009 5:30 PM
To: [log in to unmask]
Subject: Re: [TN] Adhesion Testing of Brush Plating
Joyce,
Each area being Brush Plated is a unique area and a coupon to mirror the surface being plated is not practical.
Regards,
Tom Carroll, CQA, CIT
Supplier Quality Engineer
-----Original Message-----
From: Joyce Koo [mailto:[log in to unmask]]
Sent: Wednesday, September 23, 2009 4:22 PM
To: TechNet E-Mail Forum; Carroll, Thomas A
Subject: RE: [TN] Adhesion Testing of Brush Plating
Is it suppose to be done on coupon or at qualification stage? Why you need to do every batch? If you do, why not have a witness coupon designed along your production part?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Carroll, Thomas A
Sent: Wednesday, September 23, 2009 5:20 PM
To: [log in to unmask]
Subject: [TN] Adhesion Testing of Brush Plating
Fellow Techies,
MIL-STD-865D, Selective, Brush Plating, Electro-Deposition calls for Adhesion Testing per paragraph 5.5.6e 1 (tape test) or 2 (shot peen).
But I have a supplier telling me that they do not perform the adhesion test on production application because it would leave a residue.
My question is this:
Do any of you have experience with Selective Brush Plating and if yes, would you recommend allowing the adhesion test to be waived on production hardware?
Thanks in advance for your response,
Tom Carroll, CQA, CIT
Supplier Quality Engineer
Boeing Integrated Defense Systems - East Region Supplier Quality
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|