Well, not exactly that, but knock, knock, knock on a earthly board. One
customer needs fix a intermittent problem asap. 19 inch racks with hundreds
of PTH double sided boards, old technology, no BGAs, no QFMs etc, but lots,
lots of DIPs. The edge contact fingers have a very thick and good gold over
nickel, and the backplane connectors have really stiff double tongues. The
contact pressure/sq is extremly high and I think the contact spots are
really gastight once the board is plugged in. Now, they have electrical
issues, and they've found, that the signals are interrupted or coming back
when they knock on the boards. Someone is going to take a flight the other
day to fix the problem. The electricians believe, stubborn as mules, that
the only think needed, is to take out the boards and clean the edge contact
fingers with a solvent and that will fix it. Myself, with quite many year's
experience from connectors, I don't think that is the problem, because when
such robust contact springs wipe along the contact fingers, they slide
pretty deep into the gold and makes good connection. Each spring has double
contact ridges, so the risk that some dirt should cause interrupts is
minimal. There is more that talks against their theory, namely, that the
problem is still there after plugging, deplugging more than once. I'm sure
there is a solder joint issue, or maybe a bond wire problem in the packages.
Logically, this later is more likely because you have thousands of
solder/bond joints vs, just some one hundred edge connector ditto. A ratio
like 10,000/100 per board. Without knowing all details, what is your general
experience between the index finger and the big toe?
/Inge
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|