To see or not to see, that's the question. We don't rely 100% on what we
see, so we use a indirect method, which means buying test BGAs with no chip
in, but daisy chains. After soldering them, we run environmental tests and
the following electrical tests will tell us if the concept is good enough.
Takes time, yes. Some tests are not evaluated in less than half a year, and
I understand that this is not acceptable to most people. However, if you
plan a mass production of a certain product, the mentioned way is best.
/Inge
----- Original Message -----
From: "Bev Christian" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, September 22, 2009 2:25 PM
Subject: Re: [TN] Acoustic Microscopy for Under fill Coverage
Vlad is correct, but let me elaborate. You can pop them off with a
screwdriver or other instrument of death, but it can be messy and if you are
interested in voids that don't come up to the underfill/part interface, you
may not see them that way. Planar sectioning is best. But as Dr Brian Toleno
points out in his underfill course (a little free advertising there, New
Dad), a normal vertical cross-section will show you if you have any filler
settling. This of course assumes you are using an underfill with a filler in
it. :)
Bev
RIM
----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Tue Sep 22 07:39:24 2009
Subject: Re: [TN] Acoustic Microscopy for Under fill Coverage
Amol,
Probably the only other choice you have is to grind off the package
gradually and inspect the underfill coverage.
Regards,
Vladimir
SENTEC
SENTEC
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca
-----Original Message-----
From: "Kane, Amol (349)" <[log in to unmask]>
Date: Tue, 22 Sep 2009 07:30:22
To: <[log in to unmask]>
Subject: Re: [TN] Acoustic Microscopy for Under fill Coverage
Guys, thank you for all the interest in the subject. Lots of good
information indeed. Yes, I did talk to Sonoscan and they pretty much
corroborated what most people here are saying in that there are too many
interfering layers to effectively look at underfill coverage and any voids
or dewetting to the board/component surface.
So let me ask this...HOW CAN I look at a underfilled BGA and determine how
good/bad my process for underfilling them is? (I am setting up a new process
for manually underfilling BGAs). I want to determine if the underfilling
technique used is consistently producing good results across BGAs and if the
board cleanliness level is sufficient to ensure complete wetting and spread
underneath the BGA. I am working with test vehicle now, but the actual
boards will be used in a shock application. Any established standards
(formal or informal) out there? The bottom line is that I need to be able to
show the customer that the process produces underfilled BGAs with minimal
voiding and dewetting.
Werner, are the critical areas (i.e. the corners) the same for shock/vibe as
for more gradual stresses on a BGA?
Thanks,
Amol
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Monday, September 21, 2009 11:12 PM
To: [log in to unmask]
Subject: Re: [TN] Acoustic Microscopy for Under fill Coverage
Hi Werner -- there have been a number of examples in which a component
construction interaction of a "partial underfill" has resulted in
increased degradation of the solder joint integrity in comparison to a
"complete underfill" case.
Dave
Werner Engelmaier /* <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
09/21/2009 06:17 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]
To
[log in to unmask]
cc
Subject
Re: [TN] Acoustic Microscopy for Under fill Coverage
Hi Guys,
The premise of the original question was by inference that completeness of
the underfill coverage is necessary.
Would not be an underfill 'ring' covering the first 5 or so 'SJ squares'
accomplish what is desired?better reliability? That would make this
discussion academic.
Werner
-----Original Message-----
From: Vladimir Igoshev <[log in to unmask]>
To: [log in to unmask]
Sent: Mon, Sep 21, 2009 6:47 pm
Subject: Re: [TN] Acoustic Microscopy for Under fill Coverage
C-SAM does do a beautiful work on flip-chip packages and of cause not in
the
transmission mode.
Regards,
Vladimir
SENTEC
SENTEC
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca
-----Original Message-----
From: "David D. Hillman" <[log in to unmask]>
Date: Mon, 21 Sep 2009 17:30:36
To: <[log in to unmask]>
Subject: Re: [TN] Acoustic Microscopy for Under fill Coverage
Hi Bev - I have attempted to use Acoustic Microscopy for underfill
coverage on BGAs and as other folks have detailed, the number of
interfaces and structures cause significant signal reflection problems
making analysis very difficult. Some specific focused interface
examination efforts can be conducted but are still very difficult to
analyze.
Dave Hillman
Rockwell Collins
[log in to unmask]
Bev Christian <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
09/21/2009 05:16 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond=2
0to
Bev Christian <[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] Acoustic Microscopy for Under fill Coverage
John and others,
But wouldn't it be even worse trying to use transmission mode because of
the nature if the circuit board underneath the component (copper
barrier(s), glass fiber bundles and epoxy?
Nobody from Sonotek or Sonoscan on TechNet?
Bev
----- Original Message -----
From: John Burke <[log in to unmask]>
To: 'TechNet E-Mail Forum' <[log in to unmask]>; Bev Christian
Sent: Mon Sep 21 18:00:16 2009
Subject: RE: [TN] Acoustic Microscopy for Under fill Coverage
Not a discontinuity as such just an interface, and you are right, the
signal reflections will be from every interface, so for a BGA (without a
lid) the interfaces will be as follows:
1 Liquid to top of package molding compound
2 Molding compound to silicon
3 Silicon to die attach
4 Die attach to substrate
5 4 or so interfaces in the substrate itself (copper to substrate
pre-preg)
6 Substrate to under fill (or NOT!)
Depending of the acoustic impedance between the Material travelling
from/Material travelling to, more or less ultrasound energy will be
reflected at each of the interfaces.
Of the layers above I believe that the strongest reflection will be from
level 6 above.
It is 30 years since I last played with non destruct testing using
ultrasonics, but I would bet from my experiences then that you would do
far
better using through transmission for this scenar
io rather than reflected
signals due to Bev's comment, particularly due to the substrate interface
reflections masking the ones between the package and the under fill.
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Monday, September 21, 2009 2:07 PM
To: [log in to unmask]
Subject: Re: [TN] Acoustic Microscopy for Under fill Coverage
Since when can an acoustic signal punch through a BGA? I know you can do
if
for flip chips, but aren't there too many density discontinuities for CSPs
abd BGAs?
Bev
----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Mon Sep 21 14:40:48 2009
Subject: [TN] Acoustic Microscopy for Underfill Coverage
Anybody know a good lab in the North East that does acoustic microscopy? I
need to verify under fill coverage under BGAs.
Thanks,
Amol
WARNING: Export Control
This document may contain technical data within the definition of the
International Traffic in Arms Regulations (ITAR), and subject to the
Export
Control Laws of the U.S. Government. Transfer of such data by any means
to
a foreign person, whether in the United States or abroad, without proper
export authorization or other approval from the U.S. Department of State
is
prohibited.
CONFIDENTIALITY NOTICE:
This e-mail, and any attachments, is for the sole use of the intended
recipient(s) and may contain information that is confidential and
protected
from disclosure under the law. Any
unauthorized review, use, disclosure,
or
distribution is prohibited. If you are not the intended recipient, please
contact the sender by reply e-mail, and delete/destroy all copies of the
original message and attachments.
Thank you.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from
your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authoriz
ed and may be
unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from
your system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be
unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask]
0with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
WARNING: Export Control
This document may contain technical data within the definition of the
International Traffic in Arms Regulations (ITAR), and subject to the Export
Control Laws of the U.S. Government. Transfer of such data by any means to
a
foreign person, whether in the United States or abroad, without proper
export
authorization or other approval from the U.S. Department of State is
prohibited.
CONFIDENTIALITY NOTICE:
This e-mail, and any attachments, is for the sole use of the intended
recipient(s) and may contain information that is confidential and
protected from disclosure under the law. Any unauthorized review, use,
disclosure, or distribution is prohibited. If you are not the intended
recipient, please contact the sender by reply e-mail, and delete/destroy
all copies of the original message and attachments.
Thank you.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|