Toby,
I would not see any change in OPENS. I see no means of interaction between
existence of top pour and thermal profile during reflow. Yes you have a
little more copper around the BGA.
I would be more worried about shorts if there were solder mask chips and
exposed metal due to handling or BGA rework.
Bob Kondner
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Toby Carrier
Sent: Wednesday, September 16, 2009 1:54 PM
To: [log in to unmask]
Subject: Re: [TN] Ground Pour Under BGA
What are the reliability/assembly issues to be concerned with when either
adding the pour or not? Is there a larger chance of non-soldered balls by
using either technique?
Toby
On Wed, Sep 16, 2009 at 11:56 AM, Dwight Mattix <[log in to unmask]>wrote:
> At 08:39 AM 9/16/2009, Robert Kondner wrote:
>
>> Hah?
>>
>> The wavelength of 800Mhz is 1.2 feet. So y/20 = .72 inches. Even the
>> higher harmonics are over 100 mil.
>>
>
> a little cell phone industry humor there. 800 MHz. Get it? ;^)
>
>
> The length of a via to an internal plane is about 20 mils? The is 1/5 of
>> the higher harmonics. Give me a break.
>>
>> You must be joking if you think placing a "Swiss Cheese" plane on the
PCB
>> top for saving a 10mil via distance is going to affect signal impendence.
>> That "Swiss Cheese" plane is probably a greater Z than the vias. Still
>> compared to a wavelength of 1.2 feet it is not going to be measureable.
>>
>
> Benefit is not so much for impedance as it is for distributed capacitance
> if designed to take advantage of it. Mute point in our world anyway.
> Except for emulator cards almost all of our work is on high I/O.4mm and
> .5mm pitch devices (670-1000 pins). Forget swiss cheese. There's nothing
> but fanout and hookup going on in those 6 or 9 mil routing channnels.
>
>
> Bob Kondner
>>
>>
>>
>> -----Original Message-----
>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Dwight Mattix
>> Sent: Wednesday, September 16, 2009 11:27 AM
>> To: [log in to unmask]
>> Subject: Re: [TN] Ground Pour Under BGA
>>
>> At 07:36 AM 9/16/2009, Lee Hill wrote:
>> >Ok Bob I will try to find it.
>> >Yes, the problem assumes "high frequency". F>100 MHz would be high
>> enough.
>> >And for today's technology that is pretty "low" :-)
>>
>> Hah. These days DC is about 800 MHz. /heh
>>
>> >Traditional lumped-element noise theory models capacitive coupling as
>> >"small" value of capacitance. In other words, it is "accidental",
>> "stray",
>> >or "parasitic". If it were a big value it would be obvious to the
>> designer
>> >and he/she would avoid it at all costs. The Z of the stray capacitance
at
>> >the noise frequency determines the amount of noise current injected. The
>> >impedance of the victim circuit determines the noise voltage that is
>> >developed. You mention the impedance of vias, I'm not sure what they
are
>> >but I don't think they are relevant to the E-field coupling from the
body
>> of
>> >the noisy IC to say, a nearby enclosure cover, or a wire attached to the
>> PCB
>> >a few cm away, or to data transceiver IC a few cm away.
>> >
>> >Tiny amounts of mutual inductance (picoH) and capacitance (pF) do cause
>> many
>> >noise problems. The case I was referring to above is not "electrostatic
>> >coupling", "static" implies stationary and/or "DC".
>> >
>> >Best Regards
>> >
>> >Lee
>> >
>> >-----Original Message-----
>> >From: Robert Kondner [mailto:[log in to unmask]]
>> >Sent: Wednesday, September 16, 2009 10:21 AM
>> >To: 'TechNet E-Mail Forum'; 'Lee Hill'
>> >Subject: RE: [TN] Ground Pour Under BGA
>> >
>> >Lee,
>> >
>> > If you still have any links to that research I would love to read it.
>> >
>> > Ok, I can see a electrostatic (Near Field) effect is possible, I
>> recall
>> my
>> >Hog Wash label from that effect. But as far as the chip body to board
>> >capacitance it would have to be a pretty high frequency to be less than
>> the
>> >Z of a couple 10 mil long vias. At least I think.
>> >
>> > Thanks again, it is definitely something to think about.
>> >
>> >Bob Kondner
>> >
>> >
>> >-----Original Message-----
>> >From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee Hill
>> >Sent: Wednesday, September 16, 2009 10:10 AM
>> >To: [log in to unmask]
>> >Subject: Re: [TN] Ground Pour Under BGA
>> >
>> >There was good EMC research done about 5-7 years ago at the University
of
>> >Missouri-Rolla (UMR - now Missouri University of Science and Technology)
>> >that investigated this design technique and explained how, why, and when
>> it
>> >might be helpful. I know it is tempting sometimes to dismiss seemingly
>> >weird or useless PCB EMC design techniques out-of-hand, but there are a
>> lot
>> >of smart people around the world spending a lot of time doing
>> mathematical,
>> >computational, and experimental research work to analyze, understand,
and
>> >prove the usefulness or uselessness of many different aspects of PCB
>> design.
>> >
>> >For this specific example, the basic idea is to encourage capacitive
>> >coupling from the top of the IC back down to the "low side of the
>> source",
>> >which in general is the "ground plane" of the PCB. For it to be
>> perceived
>> >as effective, many conditions must be met 1) the IC must be troublesome
>> >source of E field coupling, 2a) there must be a "victim" of the E field
>> >coupling, and 2b) the victim is sensitive enough or the regulatory
>> emissions
>> >limit low enough that the noise coupling is troublesome. "plane
>> impedance"
>> >is a little vague, it is not clear whether this refers to power bus
>> >impedance (then there must be a second power conductor somewhere), or
>> just
>> >the impedance of the ground plane(s) alone, which is not defined without
>> >first defining a complete signal or noise loop geometry. If we have a
PCB
>> >where there already is a "ground" plane at layer 2, then there probably
>> is
>> >not as much benefit to the technique for noise control. I think the
>> research
>> >was spurred by the use of 4 or 6 layer boards, where the IC might not
>> >"normally" have a "ground" plane directly beneath it.
>> >
>> >Best Regards
>> >
>> >Lee UMR '92
>> >
>> >Lee Hill
>> >
>> >SILENT
>> >10 Northern Boulevard, Suite 1
>> >Amherst, NH 03031
>> >USA
>> >+1 (603) 578-1842 (v)
>> >+1 (603) 578-1843 (f)
>> >+1 (508) 341-3947 (m)
>> >[log in to unmask]
>> >
>> >Electromagnetic Compatibility and RF Design, Troubleshooting and
Training
>> >
>> >
>> >
>> >
>> >-----Original Message-----
>> >From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner
>> >Sent: Wednesday, September 16, 2009 8:42 AM
>> >To: [log in to unmask]
>> >Subject: Re: [TN] Ground Pour Under BGA
>> >
>> >Hi,
>> >
>> > What would be the goal of placing atop side GND plane under the BGA?
>> >
>> > Low Z Gnd return? Electrostatic shield?
>> >
>> > Having a plane under the BGA vs another layer is not going to make a
>> >difference in plane Z.
>> >
>> > Sounds like a good chance of creating shorts if the solder mask chips
>> or
>> is
>> >damaged during rework.
>> >
>> >Bob Kondner
>> >
>> >-----Original Message-----
>> >From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey
>> >Sent: Wednesday, September 16, 2009 7:43 AM
>> >To: [log in to unmask]
>> >Subject: Re: [TN] Ground Pour Under BGA
>> >
>> >IPC 7095, BGA Technology by Lau.
>> >
>> >-----Original Message-----
>> >From: TechNet [mailto:[log in to unmask]] On Behalf Of Toby Carrier
>> >Sent: Tuesday, September 15, 2009 8:45 PM
>> >To: [log in to unmask]
>> >Subject: [TN] Ground Pour Under BGA
>> >
>> >Hello all,
>> >
>> >Is it a good idea to create a top layer ground flood under a BGA
package?
>> I
>> >am
>> >guessing that the fanout will not allow much area for the ground pour,
am
>> I
>> >correct in thinking so? Does anyone have any good reference info on this
>> >topic?
>> >
>> >Also, if you don't have a ground pour under the BGA, how will that
affect
>> >the
>> >impedance control of the traces going to the BGA ball?
>> >
>> >Thanks for the help,
>> >
>> >Toby
>> >
>> >---------------------------------------------------
>> >Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> >To unsubscribe, send a message to [log in to unmask] with following text
>> in
>> >the BODY (NOT the subject field): SIGNOFF Technet
>> >To temporarily halt or (re-start) delivery of Technet send e-mail to
>> >[log in to unmask]: SET Technet NOMAIL or (MAIL)
>> >To receive ONE mailing per day of all the posts: send e-mail to
>> >[log in to unmask]: SET Technet Digest
>> >Search the archives of previous posts at:
>> http://listserv.ipc.org/archives
>> >Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>> >for additional information, or contact Keach Sasamori at
[log in to unmask]
>> >847-615-7100 ext.2815
>> >-----------------------------------------------------
>> >
>> >---------------------------------------------------
>> >Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> >To unsubscribe, send a message to [log in to unmask] with following text
>> in
>> >the BODY (NOT the subject field): SIGNOFF Technet
>> >To temporarily halt or (re-start) delivery of Technet send e-mail to
>> >[log in to unmask]: SET Technet NOMAIL or (MAIL)
>> >To receive ONE mailing per day of all the posts: send e-mail to
>> >[log in to unmask]: SET Technet Digest
>> >Search the archives of previous posts at:
>> http://listserv.ipc.org/archives
>> >Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>> >for additional information, or contact Keach Sasamori at
[log in to unmask]
>> >847-615-7100 ext.2815
>> >-----------------------------------------------------
>> >
>> >---------------------------------------------------
>> >Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> >To unsubscribe, send a message to [log in to unmask] with following text
>> in
>> >the BODY (NOT the subject field): SIGNOFF Technet
>> >To temporarily halt or (re-start) delivery of Technet send e-mail to
>> >[log in to unmask]: SET Technet NOMAIL or (MAIL)
>> >To receive ONE mailing per day of all the posts: send e-mail to
>> >[log in to unmask]: SET Technet Digest
>> >Search the archives of previous posts at:
>> http://listserv.ipc.org/archives
>> >Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>> >for additional information, or contact Keach Sasamori at
[log in to unmask]
>> >847-615-7100 ext.2815
>> >-----------------------------------------------------
>> >
>> >---------------------------------------------------
>> >Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> >To unsubscribe, send a message to [log in to unmask] with following text
>> in
>> >the BODY (NOT the subject field): SIGNOFF Technet
>> >To temporarily halt or (re-start) delivery of Technet send e-mail to
>> >[log in to unmask]: SET Technet NOMAIL or (MAIL)
>> >To receive ONE mailing per day of all the posts: send e-mail to
>> >[log in to unmask]: SET Technet Digest
>> >Search the archives of previous posts at:
>> http://listserv.ipc.org/archives
>> >Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>> >for additional information, or contact Keach Sasamori at
[log in to unmask]
>> >847-615-7100 ext.2815
>> >-----------------------------------------------------
>> >
>> >---------------------------------------------------
>> >Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> >To unsubscribe, send a message to [log in to unmask] with following text
>> in
>> >the BODY (NOT the subject field): SIGNOFF Technet
>> >To temporarily halt or (re-start) delivery of Technet send e-mail to
>> >[log in to unmask]: SET Technet NOMAIL or (MAIL)
>> >To receive ONE mailing per day of all the posts: send e-mail to
>> >[log in to unmask]: SET Technet Digest
>> >Search the archives of previous posts at:
>> http://listserv.ipc.org/archives
>> >Please visit IPC web site
>> >http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>> >information, or contact Keach Sasamori at [log in to unmask] or
>> >847-615-7100 ext.2815
>> >-----------------------------------------------------
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
>> http://listserv.ipc.org/archives
>> Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>> for additional information, or contact Keach Sasamori at [log in to unmask]
>> 847-615-7100 ext.2815
>> -----------------------------------------------------
>>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16for additional information,
or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|