Dean Stadem <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
Organization:
Analog Technologies Corp
MIME-Version:
1.0
Parts/Attachments:
text/plain (112 lines)
A contributing factor, but not the root cause.

R. Dean Stadem
Consulting Engineer
Analog Technologies Corp./Lumagine, Inc.
11441 Rupp Drive
Burnsville, MN 55431
(952)894-9228
[log in to unmask]


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Edwards
Sent: Thursday, September 03, 2009 3:15 PM
To: [log in to unmask]
Subject: Re: [TN] BGA Voids

Larry,

Sounds like the reflow profile is too hot on the bottom side...

Paul

Paul Edwards

Surface Art Engineering


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Larry Dzaugis
Sent: Thursday, September 03, 2009 9:54 AM
To: [log in to unmask]
Subject: [TN] BGA Voids

I have a 5-10% void on a bottom side BGA that grows to a 20-40% void
when
the top side is assembled and reflowed.
Paste lead free OM338, profile is peak temp is 246 for 60 seconds.
Immersion tin board finish.

Why would the void expand on a second reflow? There are 22 BGA's on this
assembly. Only a few are growing voids, most voids seen are in the 5-10%
or
less range.

Two parts are in the process of cross sectioning, to verify where the
void
really is. Only have in line x-ray capablility, no angled views.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

 =======================================================================
======

This email and any attachments thereto may contain private,
confidential, and
privileged material for the sole use of the intended recipient. Any
review, copying,
or distribution of this email (or any attachments thereto) by others is
strictly prohibited.
If you are not the intended recipient, please contact
[log in to unmask]
immediately and permanently delete the original and any copies of this
email and
any attachments thereto.

 =======================================================================
======


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2