Juan: You may want to consider cleaning/deoxidizing existing silver, rather than re-plating.
Much easier/cheaper.
Rudy Sedlak
RD Chemical Company
--- On Wed, 9/23/09, Juan T. Marugán <[log in to unmask]> wrote:
From: Juan T. Marugán <[log in to unmask]>
Subject: [TN] IAg PCBs. Re-plating?
To: [log in to unmask]
Date: Wednesday, September 23, 2009, 9:06 AM
Hello,
I have a couple of questions for the PCBs specialist people.
We have a high quantity of boards plated with IAg. Most of them were
manufactured before 2008. The questions are:
Is it possible to re-activate or re-plate the boards with the same finishing
(IAg)? Risks?
Is it possible to remove the IAg and then to re-plate them with ENIG? Risks?
Thank you.
Juan T. Marugán
Indra Sistemas SA
Spain
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|