Hi Kevin,
Ag-embrittlement, as are Au-embrittlement and Pd-embrittlement, are only an issue when you have high enough plating thicknesses which cannot be achieved with immersion plating processes. Immersion plating processes are self-limiting; all other processes can be problematic.
Werner
-----Original Message-----
From: Glidden, Kevin <[log in to unmask]>
To: [log in to unmask]
Sent: Wed, Sep 30, 2009 11:28 am
Subject: Re: [TN] Immersion Silver for Class 3 Boards
Chester,
I am guessing here, but I think it was due to concerns about silver
embrittlement? If that is the case, I think that concern has proven to be a
little less likely. Do an TN archive search for a thread called "SnPbAg solder
and Immersion Silver PCBs" from Jan 2009. Also reference the accompanying
report IPC-TR-586, in which the 4-14 Plating Committee specifically researched
the effect of excess silver in solder joints. No evidence of such embrittlement
was found.
Kevin Glidden
Manufacturing Engineer
Luminescent Systems Inc.
-----Original Message-----
From: Harner, Chester [mailto:[log in to unmask]]
Sent: Wednesday, September 30, 2009 11:03 AM
To: [log in to unmask]
Subject: [TN] Immersion Silver for Class 3 Boards
The revised Immersion Silver IPC spec (4553A) indicates that Immersion
Silver is not recommended for Class 3 boards. There is no stated reason.
I have been looking into Immersion Silver for all the same reasons as
everyone else, to replace HASL for flatness etc. It looked very good
until the Class 3 problem.
Does anyone know why IAg would not be recommended for Class 3 boards?
Chet Harner Sr. Engineer Crane Hydro-AirePO Box 7722 Burbank Ca -
91510 818-526-2600 x3557
--------------------------------------------------------------------------------
We value your opinion! How may we serve you better?
Please click the survey link to tell us how we are doing:
http://www.craneae.com/ContactUs/VoiceofCustomer.aspx
Your feedback is of the utmost importance to us. Thank you for your time.
--------------------------------------------------------------------------------
Crane Aerospace & Electronics Confidentiality Statement:
The information contained in this email message may be privileged and is
confidential information intended only for the use of the recipient, or any
employee or agent responsible to deliver it to the intended recipient. Any
unauthorized use, distribution or copying of this information is strictly
prohibited
and may be unlawful. If you have received this communication in error, please
notify
the sender immediately and destroy the original message and all attachments from
your electronic files.
--------------------------------------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|