Guy,
Kudos to Lamar, Terry, and Dewey who all suggested Dynaloy to me.
After using several gallons of both, I can report:
Dynasolve 230 is particularly good with silicone. Dynasolve 100 is particularly good with acrylic. Both appear to be rather controllable. They work so well, that I suspect they are not particularly good for humans.
Although it is against the Dynaloy's recommendations, I find a 50/50 IPA/DI rinse essential.
Chris
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Temkin, Gregg
Sent: Monday, September 21, 2009 5:29 PM
To: [log in to unmask]
Subject: Re: [TN] silicone conformal coat removal
Dynaloy has 8 different chemistries meant for silicone conformal coat removal. Use at your own risk!
http://www.dynaloy.com/Products/conformal_coating_removers.html
-----Original Message-----
From: Guy Ramsey [mailto:[log in to unmask]]
Sent: Monday, September 21, 2009 6:52 AM
To: [log in to unmask]
Subject: [TN] silicone conformal coat removal
Is there a solvent that will help remove silicone coatings?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|