I would appreciate the pictures - please send to Steve.?? I have not heard of a connection between tin whiskers and CAF.? I have heard rumors that at about 6 gigahertz and above, tin whiskers act like antennas and degrade signal quality, but only a rumor - unpublished.
Denny Fritz
-----Original Message-----
From: Inge <[log in to unmask]>
To: [log in to unmask]
Sent: Thu, Sep 3, 2009 3:15 pm
Subject: [TN] BGA Pb-free, this is what I feared: Tin whiskers
We have HASL and via-in-pad. Electrical issues, disturbed signals. There were hundreds of Tin whiskers on inside of the unfilled vias, and even whiskers from solder pads circumperiphery, pointing at the nearby solder pads. I suspect that the signal failures are caused by CAFs. Have any of you seen a connection between the presence of Tin whiskers and CAF growth??
?
All BGA via-in-pads are solder mask defined. If you want photos, I can send a couple to the PA immigrant.?
?
/Inge ?
---------------------------------------------------?
Technet Mail List provided as a service by IPC using LISTSERV 15.0?
To unsubscribe, send a message to [log in to unmask] with following text in?
the BODY (NOT the subject field): SIGNOFF Technet?
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)?
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest?
Search the archives of previous posts at: http://listserv.ipc.org/archives?
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815?
-----------------------------------------------------?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|