TECHNET Archives

September 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Kenneth Wood <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 21 Sep 2009 12:49:19 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Content-Transfer-Encoding:
base64
In-Reply-To:
<005601ca3ad8$6b149b60$413dd220$@com>
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (1 lines)
The original question was removal of silicone-based conformal coatings. See the subject line.

Not a rough crowd, just engineers wanting to make sure nothing bad happens. Sorry if I came across the wrong way.





-----Original Message-----

From: Kenneth Wood [mailto:[log in to unmask]] 

Sent: Monday, September 21, 2009 11:28 AM

To: 'TechNet E-Mail Forum'; Stadem, Richard D.

Subject: RE: [TN] silicone conformal coat removal



Wow...rough crowd in here.

The original question was "Is there a solvent that will help remove silicone coatings?”

There was no mention of conformal coating...

Maybe he is removing a silicone coating from his desk or screwdriver :)

Ken



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.

Sent: Monday, September 21, 2009 11:57 AM

To: [log in to unmask]

Subject: Re: [TN] silicone conformal coat removal



Thanks. Underscores my earlier posting; refer to the IPC recommendations for conformal coat removal. Go by the industry standards. Avoid "everybody's" ad hoc toilet cleaners, unsafe chemicals, untested methods, etc.



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis

Sent: Monday, September 21, 2009 10:48 AM

To: [log in to unmask]

Subject: Re: [TN] silicone conformal coat removal



nPB is n-propyl bromide or 1-bromopropane, a substance that is 

ozone-depleting, but unfortunately unregulated under the Montreal 

Protocol. It is also a reproductive toxin, reducing sperm count and 

motility, and a neurotoxin, with anecdotal cases of severe effects. The 

US EPA have strict regulations how it can be used with recommended 

exposure values. OSHA have not officially pronounced on it. Various 

authorities have suggested exposure levels between 1 ppm and 100 ppm. My 

opinion is that a time-weighted value of 10 ppm may be OK with a ceiling 

short term exposure of 25 ppm. Every effort should be made to prevent 

evaporation into the atmosphere. Make sure that there is no skin 

contact, as it would seem that there may be considerable transdermal 

absorption and it is not known how such absorbed solvent is metabolised.



Brian



Stadem, Richard D. wrote:

> What is nPb?

> 

> -----Original Message-----

> From: TechNet [mailto:[log in to unmask]] On Behalf Of Charlie Pitarys

> Sent: Monday, September 21, 2009 9:47 AM

> To: [log in to unmask]

> Subject: Re: [TN] silicone conformal coat removal

> 

> Guy, a cold soak in nPb will work. Trade offs are with the thickness of

> the

> coating and it still may require some manual work or you could luck out

> and

> it may swell and completely lift off the substrate.

> Then of course you have the disposal issues. 

> Positives, It is relatively cheap and may suffice in this recovery

> process

> and at room temp should fare well on many components compatibility.

>   	

> ________________________________

> 	

> 

> -----Original Message-----

> From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey

> Sent: Monday, September 21, 2009 8:52 AM

> To: [log in to unmask]

> Subject: [TN] silicone conformal coat removal

> 

> Is there a solvent that will help remove silicone coatings? 

> 

> ---------------------------------------------------

> Technet Mail List provided as a service by IPC using LISTSERV 15.0

> To unsubscribe, send a message to [log in to unmask] with following text

> in

> the BODY (NOT the subject field): SIGNOFF Technet

> To temporarily halt or (re-start) delivery of Technet send e-mail to

> [log in to unmask]: SET Technet NOMAIL or (MAIL)

> To receive ONE mailing per day of all the posts: send e-mail to

> [log in to unmask]: SET Technet Digest

> Search the archives of previous posts at:

> http://listserv.ipc.org/archives

> Please visit IPC web site

> http://www.ipc.org/contentpage.asp?Pageid=4.3.16

> for additional information, or contact Keach Sasamori at [log in to unmask]

> or

> 847-615-7100 ext.2815

> -----------------------------------------------------

> 

> ---------------------------------------------------

> Technet Mail List provided as a service by IPC using LISTSERV 15.0

> To unsubscribe, send a message to [log in to unmask] with following text

> in

> the BODY (NOT the subject field): SIGNOFF Technet

> To temporarily halt or (re-start) delivery of Technet send e-mail to

> [log in to unmask]: SET Technet NOMAIL or (MAIL)

> To receive ONE mailing per day of all the posts: send e-mail to

> [log in to unmask]: SET Technet Digest

> Search the archives of previous posts at:

> http://listserv.ipc.org/archives

> Please visit IPC web site

> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

> ext.2815

> -----------------------------------------------------

> 

> ---------------------------------------------------

> Technet Mail List provided as a service by IPC using LISTSERV 15.0

> To unsubscribe, send a message to [log in to unmask] with following text in

> the BODY (NOT the subject field): SIGNOFF Technet

> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

> Search the archives of previous posts at: http://listserv.ipc.org/archives

> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

> -----------------------------------------------------

> 



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------




ATOM RSS1 RSS2