Hi Bruce - one issue you are going to encounter is that the shear data for
Sn63 is very dependant on the specimen configuration, temperature, test
speed and solder joint configuration. One data set which has some industry
acceptance is the information published in the International Tin Research
Institute Publication 656, titled "Solder Alloy Data: Mechanical
Properties of Solders and Soldered Joints". I recommend caution is using
any Sn63 shear strength data beyond a first order approximation without
some type of real world validation. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Bruce Bryla <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
09/14/2009 07:22 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]
To
[log in to unmask]
cc
Subject
[TN] SN63 Shear Strength over temp
Hello technetters I have searched the web for a table showing SN63 shear
strength over temp and have found numerous websites providing formulas.
Does anyone know where a table exists or is willing to share some data
they have collected? Any help would be greatly appreciated.
Thank you
Bruce Bryla
L3 Communications
Senior Quality Assurance Engineer
This electronic transmission, including all attachments, is directed i
confidence solely to the person(s) to whom it is addressed, or an
authorized recipient, and may not otherwise be distributed, copied or
disclosed. The contents of the transmission may also be subject to
intellectual prpoerty rights and all such rights are expressly claimed and
are not waived. Unless specifically modified by L-3
Communications/Nardaeast, the content of this electronic transmission is
to be read subject to L-3 Communications/Nardaeast standard terms of
business. This electronic transmission may be intercepted or affected by
viruses and/or malware programs and L-3 Communications/Nardaeast accepts
no responsibilty for any interception or liability for any form of viruses
and/or malware programs intoduced by this electronic transmission. If you
have received this transmission in error, please notify the sender
immediately by return electronic transmission and then immediately delete
this transmission, including all attachments, without copying,
distributing or disclosing same.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|