A fine focus for a de-tailed analysis?
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Wednesday, August 26, 2009 6:30 AM
To: [log in to unmask]
Subject: Re: [TN] x-ray to estimate solder voiding
We have a Fein Focus/Comet/Tiger x-ray system. Very pleased with it.
I have used Fein Focus systems since the mid 80's with the other Big
Blue.
Vic,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Buetow
Sent: Wednesday, August 26, 2009 7:56 AM
To: [log in to unmask]
Subject: Re: [TN] x-ray to estimate solder voiding
Yes, FeinFocus is still in business, under the name Xylon. It is now
part of the Comet Group.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
Sent: Wednesday, August 26, 2009 6:42 AM
To: [log in to unmask]
Subject: Re: [TN] x-ray to estimate solder voiding
Kevin,
Since it has not already been mentioned, you could also try Phoenix
X-Ray - http://www.phoenix-xray.com/en/products/ as an alternative to
Dage
Is Fein Focus still in business??
MIS Testing Services - in Canada http://www.miselectronics.com/index.php
My assumption is that the device is either not conducive to acoustic
microscopy, or you don't want to get the boards wet. Sonix
http://www.sonix.com/products/index.php3
and/or Sonoscan http://www.sonoscan.com/
May your joints be free of voids!
Steve C
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glidden, Kevin
Sent: Tuesday, August 25, 2009 2:29 PM
To: [log in to unmask]
Subject: [TN] x-ray to estimate solder voiding
I am looking to have a couple of PCBs x-rayed to estimate the solder
voiding on the bottom only center pad of an SMT component. Can anyone
recommend a place?
Off line answers OK.
Thank you,
Kevin Glidden
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|