You find details here:
http://www.microscope-depot.com/cameras.htm
Inge
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Queen
Sent: onsdag 5 augusti 2009 10:17
To: [log in to unmask]
Subject: Re: [TN] Microscope cameras
Sounds a good option can you send me the details please
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of S.Huetter
Sent: 05 August 2009 09:08
To: [log in to unmask]
Subject: Re: [TN] Microscope cameras
Inge wrote:
> We had several discussions about cheap solutions, remember?
> 'Professional' cameras, i.e. from the microscope manufacturers
> themselves, are very expensive. There may be a reason for that.
> However, when your budget does not fit, you are forced to make other
> choice. I found the below dealer for a chinese brand. I bought two,
> one 3 and one 5 Megapixel, got them yesterday and installed them
> immediately on a metalurgical microscope and on a stereo one. Took a
> couple of minutes. I'm very satisfied with the camera and the program.
> It can't cope with my former Nikon DXM1200, but it covers most that I
> need. And the price is 1/15 th of the cost for a professional camera.
> And the delivery is instant. And there is a whole bunch of adapters
> and other things in the box. Seems as you can mount to any microscope
> on the market.
> Smart.
>
> Inge
>
I have also tested different cameras on our metallurgical microscope and a 3 Megapixel camera was good enough. I have found no big difference between 3MP and 5MP. More important is the correct optical distance of the CCD-Chip.
This depends on the chip size (e.g. 1/2") and microscope. If you are using a eyepiece mounted camera try moving it back and forward to get best result.
If the microscope has an option for C-mount adapter (IMHO best choice), the length of the adapter has to be correct.
Simon
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
No virus found in this incoming message.
Checked by AVG - www.avg.com
Version: 8.5.392 / Virus Database: 270.13.43/2281 - Release Date: 08/04/09 18:01:00
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|