Jon,
What you have is what I have have known to be identified as a coined lead.
Quite a few radial type through hole components are converted to surface
mount application by coining (a controlled stamping that flattens the lead).
Following the coining process the leads are placed through a carrier and bent
approximately perpendicular to the original orientation. The lead is not a
gullwing and should not be considered as such. IPC-610D 8.2.6
See 8.2.6.6 Round or Flattened (Coined) Leads, Minimum Heel Fillet:
Class 1 wetted fillet evident, Class 2 Minimum Heel Fillet Height is solder
thickness plus 50% of lead thickness, Class 3 Minimum Heel Fillet Height is
solder thickness plus lead thickness. See IPC-610D for details.
Drew Meyer
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|