TECHNET Archives

August 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 5 Aug 2009 13:05:52 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Joyce Koo <[log in to unmask]>
Parts/Attachments:
text/plain (137 lines)
Victor, in my past life, used to monitoring the street width and chip outs.  Once you see the (a) the die map got more black out, (b) chip out close to the cct of the die, you give venfor a call ask for saw change or not.  Only works when you have good relationship with fab engineer, by pass all of the 'official' channels.  If you use large amount of die, it works like charm. 
--------------------------
Sent using BlackBerry


----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Wed Aug 05 11:36:24 2009
Subject: Re: [TN] die base chip outs / fractures

Steve,

   Thank you for sharing.   The current revision is G and I have B.   I
reviewed the current TM 2017 and I didn't see much as far anomalies,
cracks/fractures of the bulk silicon at the bonding area.   The device
is a power diode package, 2x, per package, To266.  It is not a flip chip
application.

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
Sent: Wednesday, August 05, 2009 8:20 AM
To: [log in to unmask]
Subject: Re: [TN] die base chip outs / fractures

Victor,

I am not sure what the IPC equivalent to MIL-STD-883 would be, but if
you
refer to 883, TM 2010 - internal visual - monolithic, or TM 2017
internal
visual - hybrid you may find what you are looking for.

My recollection is that TM 2010 may provide the most info [para 3.1.3]
although we were mostly concerned about chip-outs at the upper edge of
the
chip, nearer to the active region.  You might consider the section on
flip
chips for info as well.

If the chips are diced with a diamond saw, one seldom [if ever] sees
chipping along the bottom edge of the die unless there has been
mis-handling
of the sawn wafer while still on the frame.  Mainly, don't want cracks
going
in the direction of the active region of the chip - [personally, don't
want
to see cracks AT ALL - especially, if you can see them with a low-power
scope, etc].

We would not want to see loose bits of Si rattling around inside a
sealed
hybrid.  If over-molded, it is not so likely to move anywhere...

Interested in further detail of the chipping you are seeing.

You should be able to down-load MIL-STD-883G from
http://assist.daps.dla.mil/online/start/
Once you get the user sign-on info.  It is a ~6 Mb file

Steve


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Wednesday, August 05, 2009 8:16 AM
To: [log in to unmask]
Subject: [TN] die base chip outs / fractures

Fellow TechNetters:

   Is there an IPC documents pertaining to acceptance of anomalies with
die.   I am see small cracks/chip out at the die to die attach region.
How much chip out/ crack is allowed?

Victor,

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2