TECHNET Archives

August 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Carroll, Thomas A" <[log in to unmask]>
Date:
Mon, 24 Aug 2009 15:18:54 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Subject:
From:
Richard Kraszewski <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (113 lines)
Thanks!!! 


Rich Kraszewski
(920)969-6075

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Carroll, Thomas A
Sent: Monday, August 24, 2009 1:12 PM
To: [log in to unmask]
Subject: Re: [TN] ROSE Equivalency Factors

Richard,

You can also find them in MIL-STD-2000A Appendix C (page 71 has a good
list).

Regards,
Tom Carroll, CQA, CIT
Supplier Quality Engineer
Boeing Integrated Defense Systems - East Region Supplier Quality Home
Office Phone/FAX: 845-753-5932 Temp Office Phone at Alabama Aircraft
Indus Inc (205) 510-4783 Temp Office FAX at AAII (205) 592-0295 Boeing
Cell: 215-692-2463
email: [log in to unmask]

>	NOTE: This communication may contain privileged or other
confidential information. If you are not the intended recipient, or
believe you have received this communication in error, please do not
print, copy, retransmit, disseminate, or otherwise use the information.
Also, please indicate to the sender that you have received this e-mail
in error, and delete the copy you received. Thank you.
>	EXPORT COMPLIANCE STATEMENT:
>	"The information contained herein is or may be controlled by the
International Traffic in Arms Regulations (ITAR), 22 CFR 120-130, and
may not be exported, or disclosed to a foreign person, whether in the
United States or abroad, without prior U.S. Government written approval"

-----Original Message-----
From: Glidden, Kevin [mailto:[log in to unmask]]
Sent: Monday, August 24, 2009 11:17 AM
To: [log in to unmask]
Subject: Re: [TN] ROSE Equivalency Factors

MIL-PRF-55110 has them in the Appendix A.  Not sure if they were copied
to 31032 or not.


-----Original Message-----
From: Richard Kraszewski [mailto:[log in to unmask]]
Sent: Monday, August 24, 2009 12:08 PM
To: [log in to unmask]
Subject: [TN] ROSE Equivalency Factors

Can someone please refresh my memory and tell me which document has the
equivalency factors for the various ROSE testers? I seem to think that
it was the IPC TR 583, but I don't see them there. Believe it may have
been a Military document.

Thanks

Rich  Kraszewski


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2