Subject:
From:
Craig Sullivan <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (82 lines)
Thank you all. I suppose I should have dug into a few more documents. :)
Craig

Export Control:
This message is intended only for the addressee and may contain information
that is company confidential or privileged.  Any technical data in this
message may be exported only in accordance with the U.S. International
Traffic in Arms Regulations (22 CFR Parts 120-130) or the Export
Administration Regulations (15 CFR Parts 730-774). Unauthorized use is
strictly prohibited and may be unlawful. If you are not the intended
recipient, or the person responsible for delivering to the intended
recipient, you should not read, copy, disclose or otherwise use this
message. If you have received this email in error, please delete it, and
advise the sender immediately. 

-----Original Message-----
From: Gary Ferrari [mailto:[log in to unmask]] 
Sent: Wednesday, August 19, 2009 3:59 PM
To: TechNet E-Mail Forum; Craig Sullivan
Subject: Re: [TN] Minimum Conductor to PCB edge distance


IPC-2222
10.1.1 Edge Spacing Except for edge-PB contacts, the minimum distance 
between conductive surfaces and the edge of
the finished PB, or a NPTH, shall not be less than the minimum spacing 
specified in Table 6-1 of IPC-2221 plus 0.4
mm. PBs that slide into guides shall have a minimum external conductor 
to guide distance of 1.25 mm or minimum
electrical clearance (see Table 6-1 of IPC-2221), whichever is greater. 
Special design applications in areas such as high
voltage, surface mount, and radio frequency (RF) technology may require 
variances to these requirements. Ground and
heat sink planes may extend to the edge when required by design.

Craig Sullivan wrote:
> I can't seem to find this information in any IPC document, unless I am
> obviously overlooking it.
> 
> We have a PCB customer designed with a trace close to the board edge
> (0.013"). However, when the board is scored for depaneling, the score
width
> reduces the distance to around 0.005" - 0.007".
> 
> Can anyone recommend a reference or design guideline that specifies
> something like this? Something that may specify how close features can be
> placed to the board edge?
> 
> We have our own guidelines for DFA, and generally speaking, we've never
run
> into anything this tight where it's become a cause for concern. But
there's
> also a first time I suppose.
> 
> Thanks in advance for the input.
> Craig
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2