Cher Roland,
I would do a cross section in order to be sure.
I think that what I see as black spots are your micro vias with bad plating.
Seems to me that the final finish is absent inside and around the holes.
(what is it , anyway?)
You will have big voids in your BGA solder joints, for sure.
According to the pictures I would scrap the boards.
I am not at all sure that the micro vias have a good connection to the inner
layer.
Gaby
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of roland jaquet
Sent: Monday, July 27, 2009 6:23 PM
To: [log in to unmask]
Subject: [TN] Via-in pad acceptability
I need advise in a case where the outer layers have blind Via-in-pad (BGAs)
from lay14 to 13 and 1 to 2. Those were plated and filled-up with
non-conductive.
What is the acceptable level for non-uniformity of the capping?
I have 4 pictures to shareat following address:
http://www.pcbspecialist.com/PCBpics/RJ_00157.jpg
http://www.pcbspecialist.com/PCBpics/RJ_00158.jpg
http://www.pcbspecialist.com/PCBpics/RJ_00159.jpg
http://www.pcbspecialist.com/PCBpics/RJ_00160.jpg
From the IPC-6016 (HDI) I got relevant :
3.5.3.2 Surface Mount Lands (Area for attachment such as solder, TAB,
conductive adhesive) Defects such as nicks, dents, and pinholes along the
edge of the land (length or width) shall not exceed that identified in the
respective slash sheets.
Slash sheet says "As Specified" and there is no customer requirement..
3.6.4 Filled Vias Buried vias and/or buried microvias shall be filled and
inspected in accordance with the procurement documentation. Blind vias on
the external layers do not have any fill requirements.
The PCBs have been manufactured as Class 2.
What is your opinion?
Is there more documents I could base on for acceptability?
Thank you for your help
Meilleures salutations
Very Best Regards
Roland
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|