Hi Victor,
The 0.8mil Cu standard does not work with Pb-free for 2 reasons except for thin PCBs. Too thin for the PTH barrel integrity with those large thermal expansions for any resin with Tg<190C, and too thin for reworks.
Werner
-----Original Message-----
From: Victor Hernandez <[log in to unmask]>
To: [log in to unmask]
Sent: Wed, Jul 8, 2009 8:49 am
Subject: [TN] LF PTH, Knee copper thickness measurement
Fellow ThecNetters:
Can someone share their experience in measuring the Lead Free PTH
copper thickness at the knee for first pass assemblies and then after 1x
and 2x rework. This especially true on the solder side of the board.
I have reviewed the IPC-A-600F standard and did not find a
method/technique. I believe the preferred minimum thickness is 0.5
mils for 2x rework.
Victor,
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|