That is the one I had.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe Fjelstad
Sent: Wednesday, July 29, 2009 11:56 AM
To: [log in to unmask]
Subject: Re: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER JOINT
It was missing an "s" as in "circuits" This should work for you
_http://circuitsassembly.com/cms/magazine/95/3630_
(http://circuitsassembly.com/cms/magazine/95/3630)
In a message dated 7/29/2009 7:55:36 A.M. Pacific Daylight Time,
[log in to unmask] writes:
Unable to open provided URL address. Perhaps a block at my employer.
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier /*
Sent: Wednesday, July 29, 2009 9:50 AM
To: [log in to unmask]
Subject: Re: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER JOINT
There is something called a Gold-Embrittlement 'Calculator' at M. Lau & T.
Clifford, “Lockheed Martin Gold Calculator.xls,” see:
http://circuitassembly.com/cms/content/view/3630/95/
Werner
-----Original Message-----
From: Steven Creswick <[log in to unmask]>
To: [log in to unmask]
Sent: Wed, Jul 29, 2009 10:31 am
Subject: Re: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER
JOINT
Guy,
You might try to contact Steve Z and see if he has the time to drop it into
his site. I'm sure that it can't be all that large of a spreadsheet.
Possibly it is already buried there somewhere. I just took a quick peek
and
did not see something in that line of thought.
Steve C
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey
Sent: Wednesday, July 29, 2009 10:23 AM
To: [log in to unmask]
Subject: Re: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER JOINT
Technet does not allow attachments but I have a spreadsheet that I picked
up
from someone on Technet. It is dated 6/21/06.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Roberts, Jon (SA-1)
Sent: Tuesday, July 28, 2009 8:54 AM
To: [log in to unmask]
Subject: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER JOINT
Does anyone have or know where to find the formula for determining the
amount of percentage of gold in a SMT solder joint? Appreciate any
help, Jon
---------------------------------------------------
Technet Mail List provided a
s a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
**************Hot Deals at Dell on Popular Laptops perfect for Back to
School
(http://pr.atwola.com/promoclk/100126575x1223106546x1201717234/aol?redir=http:%2F%2Faltfarm.mediaplex.com%2Fad%2Fck%2F12309%2D81939%2D1629%2D8)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|