Hi Ioan,
Dave gave you all the references you need, but solderanility testing and real solderability of a board - very often two different things.
I usually recommend my customers to get down to the root cause of a problem.
You can send the boards to me for analysis if you want to.
Regards,
Vladimir
SENTEC
------Original Message------
From: Ioan Tempea
Sender: TechNet
To: [log in to unmask]
ReplyTo: TechNet E-Mail Forum
ReplyTo: Ioan Tempea
Sent: Jul 8, 2009 11:59
Subject: [TN] PCB Solderability issues
Dear Technos,
The PCB HASL wetting issues saga is not over. The PCB fab told me they are doing XRF on the pads. Does this have anything in common with solderability assessment?
What would be the methods of measuring solderability of HASL bare boards? And what are the pass limits?
Thank you,
Ioan Tempea, ing.
Ingénieur Principal Fabrication / Sr. Manufacturing Engineer
30 ans déjà! - Already 30 years!
950 rue Bergar, Laval, Québec, H7L 5A1
t : 450-967-7100 ext : 244
Mtl : 514-990-5762
f : 450-967-7444
[log in to unmask] <mailto:[log in to unmask]>
www.digico.cc <http://www.digico.cc/>
P N'imprimer que si nécessaire - Print only if you must
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
SENTEC
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca
|
|
|