Unless the requirement for a HASL surface finish thickness is specifically stated, the default requirement is coverage and solderable.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Wednesday, July 08, 2009 9:35 AM
To: [log in to unmask]
Subject: Re: [TN] PCB Solderability issues
Hi Ioan! You can assess the solderability of a HASL surface finish using
the IPC-JSTD-003 specification. The thickness of a surface finish has a
direct impact on the solderability and shelf life characteristics. The
JSTD-003 specification covers how to do the solderability testing. The
thickness requirement for a HASL surface finish would be in IPC-6012 or
per your internal requirements.
Dave Hillman
Rockwell Collins
[log in to unmask]
Ioan Tempea <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
07/08/2009 10:59 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Ioan Tempea <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] PCB Solderability issues
Dear Technos,
The PCB HASL wetting issues saga is not over. The PCB fab told me they are
doing XRF on the pads. Does this have anything in common with
solderability assessment?
What would be the methods of measuring solderability of HASL bare boards?
And what are the pass limits?
Thank you,
Ioan Tempea, ing.
Ingénieur Principal Fabrication / Sr. Manufacturing Engineer
30 ans déjà! - Already 30 years!
950 rue Bergar, Laval, Québec, H7L 5A1
t : 450-967-7100 ext : 244
Mtl : 514-990-5762
f : 450-967-7444
[log in to unmask] <mailto:[log in to unmask]>
www.digico.cc <http://www.digico.cc/>
P N'imprimer que si nécessaire - Print only if you must
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|