Hi Amol,
You may want to try some cleaner degreaser before applying any conformal
coating for cleanig the board.
Try this: http://www.mgchemicals.com/products/406b.html
Hetal
On Thu, Jun 25, 2009 at 12:54 PM, Kane, Amol (349) <[log in to unmask]>wrote:
> What solvents/methods are folks out there using to clean PBCs before
> conformal coating? I want to try to get away from IPA because of waste
> disposal concerns. Any alternative solvents being used that give good
> results?
>
> Regards,
> Amol
>
>
>
>
> WARNING: Export Control
> This document may contain technical data within the definition of the
> International Traffic in Arms Regulations (ITAR), and subject to the Export
> Control Laws of the U.S. Government. Transfer of such data by any means to
> a
> foreign person, whether in the United States or abroad, without proper
> export
> authorization or other approval from the U.S. Department of State is
> prohibited.
>
> CONFIDENTIALITY NOTICE:
> This e-mail, and any attachments, is for the sole use of the intended
> recipient(s) and may contain information that is confidential and
> protected from disclosure under the law. Any unauthorized review, use,
> disclosure, or distribution is prohibited. If you are not the intended
> recipient, please contact the sender by reply e-mail, and delete/destroy
> all copies of the original message and attachments.
> Thank you.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|