Subject:
From:
stephengregory5849 <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; format=flowed; charset="iso-8859-1"; reply-type=original
MIME-Version:
1.0
Parts/Attachments:
text/plain (50 lines)
Morning Denny and Everyone!

Sure, I have your picture up here:

http://stevezeva.homestead.com/files/Digital_Microscope.jpg

I must say, that is pretty slick! For the price of a modest dinner for two 
(less the bottle of wine of course) you can have that microscope. Not bad!

Steve

----- Original Message ----- 
From: "Dennis Fritz" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Saturday, July 25, 2009 9:48 AM
Subject: [TN] Digital microscope attached to regular metallurgical 
microscope to look for tin whiskers


> Steve, can you post this photo to your web page to show how we are using 
> the cheap digital microscope to look for tin whiskers.?
>
> Thanks in advance
>
> Denny Fritz, and Purdue Calumet Campus interns
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815
> ----------------------------------------------------- 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2