3 Ohms is not healthy silver epoxy joint. I've been using silver filled
adhesives for 20 years, and can say with certainty that something is wrong
when you get such a high resistance value. A normal reading is 10 milliOhms
or even lower. The resistive path consists of thousands and thousands of
silver flakes in contact with each other, and they make a low resistance
network. Are you sure of doing correct measuring? Have you followed the
curing instructions? Were the sites cleaned before application of the
adhesive? Enough adhesive dispensed?
Typical volume resistivity is some milliOhms/cm.
----- Original Message -----
From: "Eric CHRISTISON" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, July 16, 2009 10:14 AM
Subject: [TN] Silver epoxy - related question
> Interesting thread which prompts me to raise a related question.
>
> I'm using silver epoxy as part of an EMC/ESD shield. It connects a
> conductive enclosure to a PWB ground plane.
>
> Generally we get a DC resistance across the epoxy joint of about 3 Ohms.
> However after we subject a device to an ESD spike we find the resistance
> drops by maybe an Ohm or so.
>
> Anyone got an idea what's happening?
>
> Thanks,
>
>
>
> John Burke wrote:
>> Thanks to all for the replies on silver epoxy - they are as always much
>> appreciated.
>>
>> Best regards
>>
>> John Burke
>> (408) 515 4992
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
>> http://listserv.ipc.org/archives
>> Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
>> ext.2815
>> -----------------------------------------------------
>>
>>
>
> --
> Eric Christison Msc
> Mechanical Engineer
> Consumer & Micro group
> Imaging Division
>
> STMicroelectronics (R&D) Ltd
> 33 Pinkhill
> Edinburgh EH12 7BF
> United Kingdom
>
> Tel: +44 (0)131 336 6165
> Fax: + 44 (0)131 336 6001
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|