Hello Jack,
With SMOBC, I've had no problems with using solid copper for large
consuctive areas.
Certainly, it was a problem in the days with all over solder finish
under the solder mask.
I don't believe that there is any problem with the pattern plating of
the board either.
Modern LPI soldermasks adhere to the bare copper quite well also.
regards,
Phil.
________________________________
From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of Jack
Olson
Sent: Thursday, 30 July 2009 8:48 AM
To: [log in to unmask]
Subject: [DC] Hashing-Out Hatching
Greetings,
I was just reading through the latest draft of IPC-2222,
and stumbled into the advice in section 10 regarding
"large conductive areas", where we are advised to
use some kind of etched pattern (cross-hatching)
for any area larger than a 25mm diameter circle.
I have done this exactly once in the last 22 years,
does anyone else do this?
Has anyone ever experienced a problem by NOT doing
this? (not counting soldermask over HASL)
Jack
------------------------------------------------------------------------
-------
DesignerCouncil Mail List provided as a service by IPC using LISTSERV
1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in the BODY (NOT the subject field):
SIGNOFF DesignerCouncil
To temporarily stop/(start) delivery of DesignerCouncil for vacation
breaks send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext. 2815
------------------------------------------------------------------------
-------
"Warning:
The information contained in this email and any attached files is
confidential to BAE Systems Australia. If you are not the intended
recipient, any use, disclosure or copying of this email or any
attachments is expressly prohibited. If you have received this email
in error, please notify us immediately. VIRUS: Every care has been
taken to ensure this email and its attachments are virus free,
however, any loss or damage incurred in using this email is not the
sender's responsibility. It is your responsibility to ensure virus
checks are completed before installing any data sent in this email to
your computer."
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
|
|
|