Richard,
The check we do is a first article build. We build a board/panel
complete and do an in-depth inspect of this. This way if the paste has
an issue it definitely shows up because you are doing the hardest test
possible (actually making the paste do everything it needs to do).
Jerry Dengler
Production Manager
Pergamon Corporation
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Wednesday, June 24, 2009 11:01 AM
To: [log in to unmask]
Subject: Re: [TN] Solder paste validation at point of use
Richard,
At Nortel I used to do viscosity checking on every lot when it arrived.
I did that for two years and then gave it up as a waste of time.
Obviously the process engineers are doing some checking on the shop
floor, as you describe.
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Wednesday, June 24, 2009 10:22 AM
To: [log in to unmask]
Subject: [TN] Solder paste validation at point of use
I would like to know what others do to ensure that the solder paste is
good at the point of use.
I am NOT looking for a solder paste handling procedure, what I am
looking for is what type of test can be performed that is quick, easy,
and does not hold up production. We do paste viscosity testing on each
lot that we receive, and we also strictly monitor our paste printing
process with the post-print inspection machine. We have validated our
entire solder paste handling system to ensure that the paste is handled,
labeled, and properly rotated.
We have had no issues with the solder paste that we use.
Our customer thinks we should test each lot of paste when it is removed
from refrigeration prior to use on production hardware. I am not really
sure what a second viscosity check would do for us, but I am open to
some other testing method that does not consume a lot of paste and would
provide data we can use.
Any suggestions?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public information. Any use of this information by anyone other than
the intended recipient is prohibited. If you have received this
transmission in error, please immediately reply to the sender and delete
this information from your system. Use, dissemination, distribution, or
reproduction of this transmission by unintended recipients is not
authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|