No changes. I just meant that we do not change the same pcb from one
finish to the other.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lenny Carter
Sent: Wednesday, June 24, 2009 8:29 AM
To: [log in to unmask]
Subject: Re: [TN] ENIG and SN100 HASL compatability?
thanks, Larry - You mention not interchangeably but using the same
processes- are you changing anything- like profiles or stencil, etc..?
Regards,
Lenny Carter
Design Engineer
ERG, Inc.
ph (607) 754-9187 x3063
www.ergpower.com
----- Original Message -----
From: "Davis, Larry" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, June 24, 2009 8:57 AM
Subject: Re: [TN] ENIG and SN100 HASL compatability?
Hi Lenny,
We do use both finishes but not interchangeably. SN100 HASL is very
common and we are using it with great results. We typically use ENIG
when there are fine pitch pads on the board and SN100 HASL for
everything else to reduce costs. We are using the same paste, parts and
processes for each of the finishes.
Regards,
Larry
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lenny Carter
Sent: Wednesday, June 24, 2009 6:13 AM
To: [log in to unmask]
Subject: [TN] ENIG and SN100 HASL compatability?
Fellow Technetters- We design, build and ship our own electronic assys
from one lean facility in the US. 3-4 years ago went ROHS like most
others, and we settled on ENIG pcb finish and havent looked back. We
have a pcb manufacturer who wants us to try some SN100 finished ROHS
pcbs as an alternative to ENIG for the few pcbs we by from him.
I have some sample arrays to build on, but the assys are expensive and
figured I would first ask those of you who know- Is SN100 HASL finish
common? and is it fairly interchangeable with ENIG from a paste and
component finish compatibility and process perspective? Are others
readily building between SN100 & ENIG assys with little or no changes?
I understand this is a very subjective questions with many variables,
but I am posting this as a starting point.
Thanks, Lenny Carter
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
Please be advised that this email may contain confidential information.
If you are not the intended recipient, please do not read, copy or
re-transmit this email. If you have received this email in error,
please notify us by email by replying to the sender and by telephone
(call us collect at +1 202-828-0850) and delete this message and any
attachments. Thank you in advance for your cooperation and assistance.
In addition, Danaher and its subsidiaries disclaim that the content of
this email constitutes an offer to enter into, or the acceptance of, any
contract or agreement or any amendment thereto; provided that the
foregoing disclaimer does not invalidate the binding effect of any
digital or other electronic reproduction of a manual signature that is
included in any attachment to this email.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
Please be advised that this email may contain confidential information.
If you are not the intended recipient, please do not read, copy or
re-transmit this email. If you have received this email in error,
please notify us by email by replying to the sender and by telephone
(call us collect at +1 202-828-0850) and delete this message and any
attachments. Thank you in advance for your cooperation and assistance.
In addition, Danaher and its subsidiaries disclaim that the content of
this email constitutes an offer to enter into, or the acceptance of,
any
contract or agreement or any amendment thereto; provided that the
foregoing disclaimer does not invalidate the binding effect of any
digital or other electronic reproduction of a manual signature that is
included in any attachment to this email.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|