Hi Steve,
Looks like dewetting to me.
Likely scenario: Connector pins are BeCu with a Cu-flash to make them "solderable"; Cu-flash too thin and desolves essentially completely; no more solderability.
Those other to leads are not connector pins and are made of Cu.
My guess without any hard evidence.
Werner
-----Original Message-----
From: Steve Gregory <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, Jun 23, 2009 7:49 am
Subject: [TN] "Blumpie" looking connector leads...
Morning all!
Trying to stay cool here! Broke 100 degrees yesterday and Sunday, and
it's probably going to break 100 degrees today. Summer has come with a
vengeance!
Ran across something yesterday that I've never seen before. We build a
board that uses this AMP Densipac SMT connector:
http://tinyurl.com/nqbpcp
We've built a lot of these boards before without any issues at all. This
latest run we have something going on with these particular connectors.
Here's a photo of them on the PCB:
http://stevezeva.homestead.com/files/AMP_Connectors.jpg
You can probably see that the leads have this "Blumpie" look to
them...both bumpy and lumpy. This is fresh out of the reflow oven.
Here's a closer look:
http://stevezeva.homestead.com/files/Connector_Blumpies.jpg
If you notice the two pins either side of the white line look fine. They
are the anchor pins that are for mechanical strength for the
connector...they are not I/O pins. The rest of the board looks
absolutely fine too. Not a bit of problem. It's just the I/O pins. We
have noticed that connectors with certain date codes don't have this
problem. Also, before reflow the connectors look okay. Luckily we've
only built a few boards, and we're stopping until we can get to the
bottom of this...
Have any of you ever seen "blumpie" connectors like these before?
Steve
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|