We have some Immersion Tin boards that are several years old. From
everything I have read here or elsewhere, ImmSn is supposed to have a
short shelf life. 6 mos to a year. No one wants to scrap the boards
without testing them, though.
How would you verify whether they are still good? We hand-soldered some
pads and actually had no problems which surprised me, considering the
age of the boards, but I don't know if that is a valid test.
Genny
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------