I've designed a lot of boards with 2oz cu on both the internal & external
layers, I use 0,20mm spacing & 0,20mm minimum trace width. This brings the
designs into the manufacturing range of a broad range of fab shops.
Regards
Paul O' Connor CID+
---------------------------------------------------------------------------------