There has been at least one fire in a contamination tester that I know
of for certain. The company in question thereafter decreed that all
flammable solutions and products should be used only in metallic
enclosures because the PVC melted, allowing the burning solution to
spread along the floor, causing considerable collateral damage to the
workshop (I think in millions). I have heard of a possible couple of
other minor cases but nothing that I can quote chapter and verse on.
Remember that the vapours from testers are the IPA/water azeotrope and
not pure IPA. Even the small amount of water, not affecting the flash
point, does reduce the ease with which it burns.
As an ex-manufacturer of contamination testers, we took care in the
design to minimise the risk, although it can never be eliminated. I
emphasise that the one that caused all the damage was not of our
manufacture! :-o
By the same token, the bottle of Laphroaig in the CEO's cocktail cabinet
has an EtOH/water azeotrope over the liquid level, but it has a better
aroma and flavour than the contamination tester solution.
Brian
Richard Kraszewski wrote:
> We have done US cleaning using higher molecular weight alcohols and
> found them to be rather effective, especially in cleaning beneath low
> stand off components.
>
> Using lower weight and lower boiling alcohols like MeOH, EtOH or IPA
> just doesn't work well, so why even take the risk, albeit the risk is
> rather low. Remember that ROSE tester solution (~75% IPA) can get
> rather warm after awhile and I haven't heard about many (any?) fires
> related to that testing operation.
>
>
> Rich Kraszewski
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of John Anselmo
> Sent: Monday, June 29, 2009 10:27 AM
> To: [log in to unmask]
> Subject: [TN] IPA o r Methanol in Ultrasonic Cleaner
>
> Technet,
>
> We are being asked by one of our customers to clean some parts (screws,
> washers, standoffs, feedthrus) in an ultrasonic cleaner with either
> Methanol or IPA (spectroscopic grade).
> The time in the ultrasonics could be up to 1 hour.
> Does anyone else have experience and recommendations for doing this?
> My main concern is safety. What type of room or enclosure do we need
> for this?
>
> Thanks,
> John Anselmo
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|