Millions of pounds of machined parts designed for critical requirements are
cleaned daily with safe aqueous based solutions.
I am still amazed that customers dictate stone age cleaning methods with
hazardous (flammable) solvents and thinks this will suffice for a clean
substrate.
There is still some education to do. My job is safe until retirement for
sure!
John, bottom line, without an IPA designed/ready vapor degreaser already on
your floor you risk a serious fire liability. Any open top ultrasonic unit
will only generate heat and likely ignite after 1-hour. The only saving
grace is that it will evaporate before auto ignition.
Call or email me off-line if you wish to discuss this further.
Charlie Pitarys
615-983-4523
________________________________
CONFIDENTIAL
The content of this message, including any attachments, may contain
privileged and/or confidential information proprietary to Kyzen and is
intended only for the named addressees. If you are not the intended
recipient, you may not disseminate, distribute or copy this email. Please
notify the sender immediately by email if you have received this email in
error and delete this email from your system.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Anselmo
Sent: Monday, June 29, 2009 12:17 PM
To: [log in to unmask]
Subject: Re: [TN] IPA o r Methanol in Ultrasonic Cleaner
Hi Bev,
To answer your questions:
Approximately half a dozen of each (screws/washers/ etc.
The qty is for each assembly and they only need to be cleaned before final
assembly, so it will be an ongoing process.
We are trying to clean any contaminants (oils) on the machined parts.
I haven't researched what finish will be on the screws yet.
John
-----Original Message-----
From: Bev Christian [mailto:[log in to unmask]]
Sent: Monday, June 29, 2009 9:34 AM
To: TechNet E-Mail Forum; John Anselmo
Subject: RE: [TN] IPA o r Methanol in Ultrasonic Cleaner
John,
Well part of this (safety considerations) will vary from jurisdiction to
jurisdiction.
Second,
How many screws and how often? Is this once off or will it be repeating?
Third
What is it you are tying to clean off?
Fourth
Are the screws painted, chromated, etc.?
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Anselmo
Sent: Monday, June 29, 2009 11:27 AM
To: [log in to unmask]
Subject: [TN] IPA o r Methanol in Ultrasonic Cleaner
Technet,
We are being asked by one of our customers to clean some parts (screws,
washers, standoffs, feedthrus) in an ultrasonic cleaner with either
Methanol or IPA (spectroscopic grade).
The time in the ultrasonics could be up to 1 hour.
Does anyone else have experience and recommendations for doing this?
My main concern is safety. What type of room or enclosure do we need
for this?
Thanks,
John Anselmo
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|