Do realize that you are using the most selective stripper that Dynaloy
makes? This also means that it will be the least aggressive for coating
removal. You will have to extend the time and or go to a more
aggressive remover. Both Dynaloy and HumiSeal make such products. Be
sure that the your customer will finda more aggressive material to be
acceptable if you chose to go that route. The more aggressive cleaner
can also remove desired marking, so be careful there and be sure to
rinse very well, or you will have cleanliness related issues.
Controls will be key to this process.
Rich K
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Luan Nguyen
Sent: Tuesday, June 02, 2009 4:06 AM
To: [log in to unmask]
Subject: [TN] Coating tripping method.
Hi Technet,
We are having a problem concern to trip coating. Details such as:
Material: Humiseal 2A64 Part A
Humiseal 2A64 Part B
Thinner 64
Dynaloy Dynasolve 190 (GEL 190)
Mixer 200 gram Humiseal 2A64 Part A and 200 gram Humiseal 2A64 Part B,
stir them , after pour 75 gram Thinner 64 to this mixer.
Viscosity: 20 seconds.
Method: Using Dynaloy Dynasolve 190 to strip coating on PWA (Immerse
PWA into Dynaloy Dynasolve 190 about 2 hours)
We can not strip the coating layer by this method.
Would you please help us to solve this problem.
Thanks and best regards,
***************************
Nguyen Hoang Luan
QC&Training Supervisor
Spartronics VietNam Co, Ltd.
No.3, Street No.6, VSIP
Th An Dist., BDuong Prov., VN
Tel: (84-650) 784 890
Fax: (84-650) 784 891
Mobile: 090.3.667448
Email: [log in to unmask]
***************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|